Fused NaCl Electrolysis - White smoke
What is the dense white smoke that is evolved during electrolysis of fused NaCl? I've read that it's sodium peroxide/oxide and read elsewhere that
it's just NaCl. I collected some and bubbled it through water thinking I'd have a dilute NaOH solution but the pH is neutral. So is it just saline?
Tom
|
|
The WiZard is In
International Hazard
Posts: 1617
Registered: 3-4-2010
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by m1tanker78 | What is the dense white smoke that is evolved during electrolysis of fused NaCl? I've read that it's sodium peroxide/oxide and read elsewhere that
it's just NaCl. I collected some and bubbled it through water thinking I'd have a dilute NaOH solution but the pH is neutral. So is it just saline?
Tom |
Well.... like the yellow stuff in chicken shit ... yellow chicken shit...
perhaps it's sodium chloride vapour. Nothing a little silver nitrate
couldn't reveal.
[Edited on 31-1-2011 by The WiZard is In]
|
|