Dow Corning Vacuum Grease Cleanup
Anybody know a good solvent to remove Dow Corning High Vacuum Grease from glass after use?
|
|
bahamuth
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 384
Registered: 3-11-2009
Location: Norway
Member Is Offline
Mood: Under stimulated
|
|
I've had luck with KOH in Ethanol in the past instead of using expensive solvents.
Really not tried much else when I come to think about it...
Any sufficiently advanced technology is indistinguishable from magic.
|
|
rrkss
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 193
Registered: 18-12-2009
Member Is Offline
Mood: No Mood
|
|
One of my collegues reccommended Dow Corning OS-2 as a simple solvent to remove silicone grease. Going to try that first before I resort to a more
aggressive KOH Ethanol Bath. Thanks for the response.
|
|
rrkss
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 193
Registered: 18-12-2009
Member Is Offline
Mood: No Mood
|
|
Was experimenting with various solvents I had on hand and surprisingly this stuff is perfectly soluble in Ethyl Acetate. Was able to clean my joints
to a nice frosty color in a matter of seconds using Ethyl Acetate. Thought I'd share since this is a cheap and simple solvent.
|
|
smuv
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 842
Registered: 2-5-2007
Member Is Offline
Mood: Jingoistic
|
|
chlorinated solvents, THF, acetone, ethyl acetate (in order of decreasing effectiveness). It also comes out in base bath but alcohols aren't the best
solvents for it.
"Titanium tetrachloride…You sly temptress." --Walter Bishop
|
|
UnintentionalChaos
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline
Mood: Nucleophilic
|
|
Remove as much as humanly possible with paper towels/cotton swabs/pipe cleaners, then swab out with hexanes or similar. At least, this was lab
protocol when I was doing undergrad research. Acetone is the solvent of choice for apezion, IIRC.
[Edited on 6-28-10 by UnintentionalChaos]
Department of Redundancy Department - Now with paperwork!
'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
|
|
peach
Bon Vivant
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1428
Registered: 14-11-2008
Member Is Offline
Mood: No Mood
|
|
Funny I should find this topic by chance.
I just got my DuPont Krytox high vacuum grease through, which is a perfluorinated polyether thickened with their own magical Teflon.
Works like a superstar on the tapers.
Cleaning it back off is another thing. 98% sulphuric, white hot concentrated KOH, every solvent I have to hand... nothing. It needs mechanically
wiping off for the most part, the bulk will never shift with chemical methods, as per the writing on the tin (which is actually a plastic tube, and
it's not written on there...).
That's also a neat feature, as it's gradually filling the microscopic ridges in the taper grind, making them seal even better.
$100 a 2oz tube. Mmmmm....
Sorry, I'm gear whoring and boasting.
|
|
BromicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
UnintentionalChaos has it right on, wipe off as much grease as you can. Paper towels are cheap by comparison to solvents, wipe the joints until they
feel dry almost. Then use any non-polar solvent, hexanes, pet ether, toluene, xylene, MTBE, and chlorinated solvents, these things work great.
Acetone works pretty good too as well as EtOAc. MeOH doesn't work very well. Best of luck!
|
|
entropy51
Gone, but not forgotten
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1612
Registered: 30-5-2009
Member Is Offline
Mood: Fissile
|
|
No need to explain. Perfectly obvious even to us common folk who realize that silicone grease works just as well and is cheaper.
|
|
peach
Bon Vivant
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1428
Registered: 14-11-2008
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by entropy51 ![](images/xpblue/lastpost.gif) | No need to explain. Perfectly obvious even to us common folk who realize that silicone grease works just as well and is cheaper.
|
Damn commoners everywhere, YUCK! ![:P](./images/smilies/tongue.gif)
Silicon probably does work as well for most things, but I doubt DuPont would make Krytox if there wasn't a benefit to it; e.g. being sure there are
essentially zero side reactions possible due to grease interaction. Needless to say, this upperchum didn't pay $100 for his tube.
I was having a read of Dow Cornings history on their site. Lots of interesting stuff in there. Personally, I prefer the helping premature babies
stories over the luxury cars and military uses. I note they were the guys who started producing silicone insulated wire. If you've not used it before,
you're missing out. The wires drape and flex like they're made of cooked pasta.
And I was reading the silicone wiki about the curing process producing acetic acid. I knew it was involved somewhere, given the delicious salt and
vinegar crisps smell around freshly sealed bathrooms, but only just found out it's a product of the cure.
Now get off my lawn, proles!
|
|
entropy51
Gone, but not forgotten
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1612
Registered: 30-5-2009
Member Is Offline
Mood: Fissile
|
|
Quote: Originally posted by peach ![](images/xpblue/lastpost.gif) | Silicon probably does work as well for most things, but I doubt DuPont would make Krytox if there wasn't a benefit to it; e.g. being sure there are
essentially zero side reactions possible due to grease interaction. | Krytox is used mostly in special
applications such as uranium enrichment where the lubricants come into contact with UF6.
|
|
peach
Bon Vivant
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1428
Registered: 14-11-2008
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by entropy51 ![](images/xpblue/lastpost.gif) | Krytox is used mostly in special applications such as uranium enrichment where the lubricants come into contact with UF6. |
Holy moley bat boy! I better reinforce the roof of the house before I get bunker buster bombed below brown, baron, burials beneath!
I bought it because I found some for the same price as regular vacuum grease, and DuPont say the high vacuum Krytox works great for laboratory
glassware applications, which is does.
|
|
aonomus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 361
Registered: 18-10-2009
Location: Toronto, Canada
Member Is Offline
Mood: Refluxing
|
|
Quote: |
And I was reading the silicone wiki about the curing process producing acetic acid. I knew it was involved somewhere, given the delicious salt and
vinegar crisps smell around freshly sealed bathrooms, but only just found out it's a product of the cure. |
There are acetic acid curing silicones, there are methoxy curing silicones, and other types as well. The general acetic acid silicones from the
hardware store are fine for most things, but they do a real number on any exposed copper, that is where the methoxy cure silicone comes in.
As for removing silicone grease, I have never really been able to get it to go into solution in a solvent. The best I have done is paper towel wetted
with acetone, a quick wipe against a quickfit joint, and bang, its clean (enough). I suppose if you had conditions where even *slight* contaminants
would ruin your reaction, you would have to try to solvate the grease. On the other hand, finger prints would do more harm at that point, and you
would probably run the glassware through piranah solution (note: don't do this, its too dangerous!)
|
|
peach
Bon Vivant
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1428
Registered: 14-11-2008
Member Is Offline
Mood: No Mood
|
|
[gets his pen out]Anomus says... make... piranha... solution...[/bang]
I haven't upgraded to piranha cleaning yet. 98% sulphuric is current working great for sintered filter funnels, after a few washes, and sticking the
spray gun on the hose into the drip tube to blow it through the frit. I've, retardedly I now see, used strong KOH to clean sintered frits before, than
wondered why they fell apart. KOH is fine for solid borosilly glass. But the tiny bonds between the grains in a sinter rot away and it falls apart
over time. It's acid or solvents as far as they're concerned.
Another stupid mistake I've made in the past is adding KOH crystals to the glass and then the water. Or dripping it through a funnel such that bits of
crystal end up in the glass. It's not an issue, for me, in terms of it splashing back. But it does superheat the glass in one spot as it dissolves,
which causes some of it to crack; albeit, the shitty no name glass I've had thus far.
But I have run into numerous problems where they'll require multiple 98% sulphuric, hot saturated KOH and solvents to shift them, alternating between
all three and a small weapons grade supply of scrubby brushes on sticks to harass the culprit from within. So I piranha may be the dangerous route
forward.
I've broken a fair bit of glass during cleaning, because I've had to wash and rinse it so many times. Provided I can safely handle the piranha, that
may help deal with that.
I have heard first hand accounts of glass exploding when people have carelessly poured it over glass coated with organic solvents and such; e.g. their
sintered filter funnel.
I get your drift about the finger prints, but I rarely poke my fingers inside the glass. Well, they won't even fit inside the smaller
stuff, and I'm not a porker. But I have watched things like DCM rinsing the tapers clear of grease as it goes past.
It's not so much of a problem when you're reasonable sure something should work, or won't be harmed by it. But, when I'm experimenting with something
I have no real support on, it's another thing to add to the long list of variables that need squashing down as low as possible.
|
|
entropy51
Gone, but not forgotten
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1612
Registered: 30-5-2009
Member Is Offline
Mood: Fissile
|
|
Quote: Originally posted by peach ![](images/xpblue/lastpost.gif) |
I've broken a fair bit of glass during cleaning, because I've had to wash and rinse it so many times. | Handling and washing glassware without breaking it is a basic skill of the chemist. You might want to pick up that skill before
trying piranha acid, which is never actually needed if you know how to clean glassware.
|
|
peach
Bon Vivant
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1428
Registered: 14-11-2008
Member Is Offline
Mood: No Mood
|
|
Cleaning a beaker or simple flask is quite a lot easier than cleaning micro-distillation or sinter glass, you've got me beat there if that's your
point. You don't know what kind of glass I'm cleaning, what kind of environment I have to do it in, how often I'm doing it, what's in the glass or any
of the other variables.
Are you drunk tonight? Hence the replies? Hopefully.
|
|