Zinc Oxide used for Desulfurisation of feedstock gases
Does anybody know if the ZnO filters used in the petrochemical industry to remove hydrogen sulfide from feedstock gases, in the gas to liquid
processes can be treated to remove the sulfur and reused or do they have to buy more ZnO after the filters become saturated with sulfur in this
reaction?
ZnO + H2S ------> ZnS + H2O
(I'm asking cause I'm interested in building a small 'hobby' sized system to make some fuel by this and similar methods, and yes I already know it
won't be easy)
|
|
Picric-A
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 796
Registered: 1-5-2008
Location: England
Member Is Offline
Mood: Fuming
|
|
The ZnS can be burnt in air, releasing SO2 and reforming ZnO.
The SO2 is then bottled and sold.
2ZnS + 2O2 --> 2ZnO + SO2
|
|
DJF90
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline
Mood: No Mood
|
|
I'm pretty sure the SO2 will not be bottled and sold, but directly used as feedstock for the Contact process.
|
|
Picric-A
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 796
Registered: 1-5-2008
Location: England
Member Is Offline
Mood: Fuming
|
|
why transport large quantities of ZnS to the contact plant when it can be burnt and reused in-situe and selling the SO2? SO2 is used in vast
quantities for making bleaches ect...
TBH it depends on how close the two plants are...
|
|
DJF90
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline
Mood: No Mood
|
|
I was making a point...
|
|
Hanfgeist
Harmless
Posts: 5
Registered: 5-12-2008
Location: Scotland
Member Is Offline
Mood: No Mood
|
|
guys,
Thanks for the most informative replies
|
|
watson.fawkes
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2793
Registered: 16-8-2008
Member Is Offline
Mood: No Mood
|
|
I would be curious to know if ZnO filter can be reconditioned in place without losing its mechanical stability. I would image that it would require a
mechanical reactant support, and possibly a mixture with a chemically-passive oxide or salt to lower the melting point in order to it in liquid phase.
If so, such a filter could be used in a twin-tank arrangement, where they switch between filtration and reconditioning. (This is how some air
desiccators work.)
|
|
Hanfgeist
Harmless
Posts: 5
Registered: 5-12-2008
Location: Scotland
Member Is Offline
Mood: No Mood
|
|
I have been doing some further reading on the subject of feedstock gas 'sweetening' and it seems that you can also use 'amines' like monoethanolamine
(MEA) to remove H2S from the input gas stream. It can then be released from the amines and passed through a Claus process plant to recover most of the
elemental sulphur......
|
|