[*] posted on 26-12-2003 at 06:16
I need something that will form a strong bond with plastic...


One of the wheels on my slide out garbage can broke. I've tried glueing it together with everything. Anyone know something that will fix it?



View user's profile View All Posts By User
Organikum
resurrected
*****




Posts: 2337
Registered: 12-10-2002
Location: Europe
Member Is Offline

Mood: frustrated

[*] posted on 26-12-2003 at 06:54


what plastic is it?

Somewhere on the garbage can has to be a something telling you what plastic it is:
For example a triangle with PP or PE written in it - look and tell.

No sign no repair. period.




Irgendwas is ja immer
View user's profile View All Posts By User
Acid Test
fruitcake
*




Posts: 48
Registered: 6-1-2004
Location: Peterborough,Ontario,Canada
Member Is Offline

Mood: Flying High Aga

[*] posted on 7-1-2004 at 12:00


Actually you could probably make a polymer
from gamma-hydroxy-butryic acid.
I know this is possible because it is a
commen procedure for the SAAB and Volvo
plants in Finland and Sweden




.....
View user's profile View All Posts By User
Haggis
Hazard to Others
***




Posts: 238
Registered: 1-12-2002
Location: Mid-America.
Member Is Offline

Mood: Lacrymating

[*] posted on 7-1-2004 at 12:22


Try Gorilla Glue. It will bond most anything especially if it is porous, like plastic that has been broken. Clean off all the glue possible, and clamp the desired items together. Just follow instructions on the bottle. The glue is expensive, and trash bins arn't that expensive, a cheap trash can can be had for, say, $8.44 at hardware stores that could fix your problem, and a new wheel to be mounted could get you off even cheaper. This isn't really mad science, but, oh well.



Great ideas often receive violent opposition from mediocre minds.
<b> <a href=\"http://pgp.mit.edu:11371/pks/lookup?op=get&search=0xEE41A2B1\">PGP Key</a> </b> 0C0A 7486 B97F 92EE AE50 A98C A4F3 087E 8CE9 A782
View user's profile View All Posts By User This user has MSN Messenger
Acid Test
fruitcake
*




Posts: 48
Registered: 6-1-2004
Location: Peterborough,Ontario,Canada
Member Is Offline

Mood: Flying High Aga

[*] posted on 7-1-2004 at 12:25


I would think that making a polymer from GHB
would be more effective.You could smear the
newly made polymer onto the crack before it
hardens.




.....
View user's profile View All Posts By User
tom haggen
Hazard to Others
***




Posts: 488
Registered: 29-11-2003
Location: PNW
Member Is Offline

Mood: a better mood

[*] posted on 7-1-2004 at 18:15


steal the wheel off your neighbors garbage can. just kiddin. man i cunt believe your trying to fix a plastic wheel. If I were your garbage man, and I saw that you had fixed your plastic wheel I would bust it off for fun. I have worked as a garbage man before.



N/A
View user's profile View All Posts By User This user has MSN Messenger
Hermes_Trismegistus
National Hazard
****




Posts: 602
Registered: 27-11-2003
Location: Greece, Ancient
Member Is Offline

Mood: conformation:ga

thumbup.gif posted on 11-1-2004 at 22:21
Vinyl Mender?


http://www.sciplus.com/category.cfm?subsection=12&catego...



Arguing on the internet is like running in the special olympics; even if you win: you\'re still retarded.