Contact Process With CO/CO2 Rich Gas


I need some soft lead for gasket material for my HF retort, so I am getting back to my lead refining project. I just set up a lead sulfating battery this evening; the full scale version of my prior experiments on using AC electrolysis in sulfuric acid to rapidly sulfate lead scrap in order to separate and purify the main metals contained therein.

The sulfates of lead, tin, and antimony are easily separated from one another due to their solubility characteristics. The final step in winning the purified metals is to smelt the sulfates with coal or coke. This releases carbon monoxide or dioxide as well as sulfur dioxide according to, for example, the reaction PbSO4 + 2C --> Pb + 2CO + SO2. Since the gas from the smelter will be extremely hot, it would be ideal to catalytically oxidize it with the Contact Process directly as it comes out, as opposed to going through any other steps of condensing the SO2 or chemically absorbing it as bisulfite or the like. However I am worried about the carbon monoxide or dioxide in the gas either poisoning the catalyst by reducing it, or interfering with the SO2 --> SO3 oxidation. I'm not sure if this will be a problem at all or not.




The mind cannot decide the truth; it can only find the truth.
View user's profile View All Posts By User
not_important
International Hazard
*****




Posts: 3873
Registered: 21-7-2006
Member Is Offline

Mood: No Mood

[*] posted on 15-7-2008 at 20:51


Don't think that will be a problem with vanadium based catalysts and an excess of oxygen.
View user's profile View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 15-7-2008 at 23:25


SO3 is a bit of an oxidizer, ain't it? Should be no problem to get rid of the CO quite rapidly then. Just use more O2.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
ShadowWarrior4444
Hazard to Others
***




Posts: 226
Registered: 25-4-2008
Member Is Offline

Mood: Sunlight on a pure white wall.

[*] posted on 16-7-2008 at 01:22


It certainly doesn’t seem that any troublesome C-S compounds can form--far too much oxygen around.

You may want to check whether your catalyst has any incompatibilities with CO or more prevalently CO2 at high temperature.

Naturally I shouldn't need to mention having adequate ventilation, gas-pressure controls, and condensation apparatus.




A bit of my photography (usually chemisty/physics inspired): ShadowWarrior4444.deviantart.com/gallery
View user's profile Visit user's homepage View All Posts By User
kilowatt
Hazard to Others
***




Posts: 322
Registered: 11-10-2007
Location: Montana
Member Is Offline

Mood: nitric

[*] posted on 22-7-2008 at 18:35


I have collected some lead salt from my sulfating battery and have been assembling the process reactors. I have the V2O5 reactor tube more or less assembled, and am using the same steel retort that I made for HF production as the smelter. The lead salt I have obtained appears to be a mixture of lead dioxide and lead sulfate. It is light grey in color overall, and contains dark colored flakes of lead dioxide. With the lead dioxide content the heat of the smelting should release some oxygen, but this will likely oxidize carbon or CO before it ever makes it to the catalyst tube, plus the rate at which oxygen is released will not be uniform for the duration of the process.

I am concerned with how I'm going to control the air feed rate since I don't know at all what rate the smelting gas will come off. I realize that excess air is not a problem for the reaction, but a great deal of excess air will dilute the already diluted smelt gas and this will slow the SO2 --> SO3 oxidation possibly to a point where the yield is very poor. A great excess of air would also carry away a lot of heat and make the process less efficient.

Another possibility is to use the pressure of the feed air (up to 100psi) to liquefy the SO2 with a condenser and separate it from CO2 and CO. The SO2 would be collected in a reservoir as CO and CO2 are vented out with a needle valve. The SO2 could then be released later to the catalyst at a more controlled rate with a needle valve. This would effectively waste all the heat carried over from the smelter as the SO2 would need cooled down to near room temperature before it would liquefy. It would however allow SO2 to be used in other processes.




The mind cannot decide the truth; it can only find the truth.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 21-8-2008 at 05:50


Quote:
kilowatt said:
I am worried about the carbon monoxide or dioxide in the gas either poisoning the catalyst by reducing it

and then later said:
Another possibility is to ... liquefy the SO2 with a condenser and separate it from CO2 and CO
Carbon monoxide is a pretty effective reducing agent. Its action on iron oxides is one of the reasons you can smelt iron in a cupola, which is charged with alternating layers of coke and iron. If not, you'd get huge oxidation losses. Now granted it's pretty hard to push straight air hard enough through the stack to get to this regime, but when you use oxygen injection to raise the melt temperature, you do get higher losses.

So, I'd guess that the action of CO in vanadium oxide would lead to greatly reduced catalyst life. With a sensitive-enough balance, a large-enough charge, and an encapsulated catalyst cell, you could just measure the mass loss by running hot CO through it. For such an analytical test, though, don't include SO<sub>2</sub> because adsorption will interfere.

You likely will have to separate out the CO. In addition to refrigeration, you could also use a scrubbing stack with a sacrificial reductant, like, say, iron oxide. This way you can keep the stack insulated and not lose the exhaust heat. The problem with designing such a stack is how to get the material in intimate contact with the gas. Solids are problematic from a surface-area vs. dust-entrainment tradoff. A spray tower might be useful.