Drying Machine Ball Mill Anyone?
So i had this idea last night...
Why not, rather than going through all the trouble of building a ball mill, just take the coffee can or ball milling container that your using, put it
in a big plastic jar for protection (both it and your drying machine) and put it in your drying machine for a few hours at a time. Might not be very
energy efficient, but if your not paying the bills...![;)](./images/smilies/wink.gif)
Just a thought....
Chemkid
[Edited on 23-4-2008 by chemkid]
|
|
CyrusGrey
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 123
Registered: 20-1-2007
Location: USA
Member Is Offline
Mood: Oooh! Shiny!
|
|
Wouldn't you waste a bunch of water doing that? Though you could put it in a drier on fluff or whatever its called (No heating tumbling).
Now what would be really neat is converting the entire drier into one giant ball mill!
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
"Now what would be really neat is converting the entire drier into one giant ball mill! "
How about an electric cement mixer? Harbor Fright has one for $100. You could use cue balls from the local tavern and a plumbers plug over the open
end. Use it to make Pd/C at a reasonable scale! ;^)
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
chemkid
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 269
Registered: 5-4-2007
Location: Suburban Hell
Member Is Offline
Mood: polarized
|
|
Meant to say dryer. Converting the entire drying machine would be interesting. I was originally using a drying machine motor for my first ball mill
(which failed and was total overkill) Anyway, i think this method might work, provided its not too loud.
|
|
tumadre
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 172
Registered: 10-5-2005
Member Is Online
Mood: No Mood
|
|
The 20 gauge sheetmetal isn't going to hold up IMO
|
|
Mr. Wizard
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1042
Registered: 30-3-2003
Member Is Offline
Mood: No Mood
|
|
I have used a cement mixer as a ball mill. I was cleaning the rust out of a gas tank. I padded the tank with some old carpet padding, taped up the
holes and threw in some old nuts and bolts and let it run for an hour. I put it on the dump position, which makes the drum horizontal. The rust that
came out was like dust. This was a very noisy operation. BTW it was a Harbor Freight mixer. It really is overkill for small jobs, and not suited for
long , or unattended operation.
After the gas tank was cleaned, some extra holes were revealed and soldered up, while the tank was flushed with CO2.
Edit: You can usually buy cast iron (steel?) balls where they sell steel and metal supplies. They are used for decorative fence and artistic metal.
[Edited on by Mr. Wizard]
|
|
Nick F
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 439
Registered: 7-9-2002
Member Is Offline
Mood: No Mood
|
|
I've used a tumble drier before, it works great. Just disable the heater and fan first.
|
|
MagicJigPipe
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1554
Registered: 19-9-2007
Location: USA
Member Is Offline
Mood: Suspicious
|
|
Most dryers (at least all the ones I have ever had) should have an air dry or "tumble" setting that will disable the heater. I don't know why you
would have to disable the fan unless you were putting what you want to mill directly inside the dryer (instead of inside some kind of cylinder).
I see no reason why it shouldn't work if you pad the cylinder good enough. You could probably even throw in some clothes to reduce the noise. Also,
on this setting, electricity use is usually less than $1 an hour. In fact, it shouldn't be more than a few kilowatt hours per mill session.
Those are just estimates and, of course, it will vary from dryer to dryer but it's not that bad. Shouldn't be any worse than running your microwave
on defrost for a few hours.
[Edited on 4-24-2008 by MagicJigPipe]
"There must be no barriers to freedom of inquiry ... There is no place for dogma in science. The scientist is free, and must be free to ask any
question, to doubt any assertion, to seek for any evidence, to correct any errors. ... We know that the only way to avoid error is to detect it and
that the only way to detect it is to be free to inquire. And we know that as long as men are free to ask what they must, free to say what they think,
free to think what they will, freedom can never be lost, and science can never regress." -J. Robert Oppenheimer
|
|
tumadre
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 172
Registered: 10-5-2005
Member Is Online
Mood: No Mood
|
|
If electricity is really expensive where you live, ie. Cali. you could put a permanent magnet or universal motor in place of the existing one.
At that level of power, the efficiency is so low for common 1/4th Hp type induction motors that replacing it with a smaller one wouldn't necessarily
reduce the consumption.
MagicJigPipe: "Shouldn't be any worse than running your microwave on defrost for a few hours." Thanks man you just made my day.
-Take it easy.
|
|
chemkid
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 269
Registered: 5-4-2007
Location: Suburban Hell
Member Is Offline
Mood: polarized
|
|
If i ever finish with all this damn school stuff I'll try this out with aluminum turnings to powder and report back....
Chemkid
|
|
chemrox
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2961
Registered: 18-1-2007
Location: UTM
Member Is Offline
Mood: LaGrangian
|
|
I was kidding about the cement mixer and assumed the dryer comments were jocular as well. I heard that aluminum foil could be turned to powder in a
blender and wonder, seriously, if the Waring technique could work for your turnings?
"When you let the dumbasses vote you end up with populism followed by autocracy and getting back is a bitch." Plato (sort of)
|
|
Phosphor-ing
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 245
Registered: 31-5-2006
Location: Deep South, USA
Member Is Offline
Mood: Inquisitive
|
|
I have also heard that small pieces of Al foil could be powdered in a blender full of NaCl. Carefully though, most blenders will not survive more a
second at a time with that kind of resistance!
"The nine most terrifying words in the English language are: 'I'm from the government and I'm here to help.'" -Ronald Reagan
|
|