Quote: | Originally posted by Fleaker
I would save your PdCl2 for more fruitful things, like palladium on carbon. NERV and I are doing an Illustrated guide on making Pd/C. In general, you
can treat Pt and Pd as equals. If you're still dead set on making a mirror, I suggest adding hydrazine sulfate to an ammoniacal solution of the PdCl2.
|
I assume the plating begins upon the addition of the hydrazine, but i now must make hydrazine sulfate.
|
|