kamal
Harmless
Posts: 33
Registered: 14-9-2005
Member Is Offline
Mood: always happy
|
|
Fibers from green Bamboo
Hi friends...!!
Can I get some suggetions from you friends for making (separating) fibers from a bamboo ? It is a cellulosic material & generally being made
commercially thro' like rayon making process & also thro' some mechanical process like crusing, grinding, etc....
However, I'm not having details about any of these proceses.
Is it possible to make suluble the fibers in something & then extracting/separating....??
I will be eagerly awaiting your suggetions.....
|
|
DrP
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 625
Registered: 28-9-2005
Member Is Offline
Mood: exothermic
|
|
I would suggest soaking them and grinding somehow. Then maybe leaving them for a while to soak some more at temperature before grinding them to a
pulp. Might be usful to boil your mix up to help break it all down. Wood fibres are made this way (high temp and grinding of a mulch) so I guess it
should be simular.
I don't know a chemical way. Certain nonylphenolethoxylates are sometimes used to break pulps down over time - I guess they could work for bamboo
as well?
What are you going to add them to?
[Edited on by DrP]
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Soaking in water followed by steam explosion is a preferred method, I believe. Bamboo is more difficult than many other fiber plants to process,
because of the hard nodes and higher silica contend; not to mention the ecologists and wildlife preservationists who will protest the destruction of
the forests and organise boycotts of your company. Industrial hemp is much easier to deal with.
From my bookmarks:
http://www.inbar.int/publication/txt/INBAR_Working_Paper_No4...
http://cat.inist.fr/?aModele=afficheN&cpsidt=1249946
http://cat.inist.fr/?aModele=afficheN&cpsidt=14887044
http://www.bc.com/environment/positionNonwood.jsp
http://www.freepatentsonline.com/5718802.html
|
|