UnintentionalChaos
International Hazard
Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline
Mood: Nucleophilic
|
|
Stability of Chromium Salts in Aqueous Soln.
The situation is simple. I dissolved some stainless steel into sulfuric acid by electrolysis and precipitated everything with NaOH. Now, I presumably
have a heap of iron hydroxide, chromium hydroxide and nickel hydroxide. I am aware that redissolving this stuff and aerating will expel the majority
of the iron salts as Fe(OH)3. If I'm not mistaken, Nickel is also stable in solution, much like copper (II). My only question is if chromium salts
hydrolyze anywhere near as easily as the iron/ Is letting the iron "rust" itself out of solution a feasile method of seperation? I have a nice heap
of brown sludge awaiting separation and will (hopefully) have some chromium salts to play with (Also making nickel salts seperately from this, so the
focus is on salvaging the chromium).
Department of Redundancy Department - Now with paperwork!
'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
|
|
guy
National Hazard
Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline
Mood: Catalytic!
|
|
Oh cool, stainless steel has a minimum of 16% Cr. Im gonna start extracting that stuff!
Cr(OH)3 will dissolve in excess NaOH. K = 8×10<sup>29</sup>
http://www.public.asu.edu/~jpbirk/qual/qualanal/chromium.htm...
Also has 10% Ni, which can be removed by ammonia.
|
|
12AX7
Post Harlot
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
Could also fuse the mixed oxides with KOH and an oxidizer (KNO3 preferred) and leach the chromate. Assuming it doesn't form an insoluble iron or
nickel chromate.
Tim
|
|
UnintentionalChaos
International Hazard
Posts: 1454
Registered: 9-12-2006
Location: Mars
Member Is Offline
Mood: Nucleophilic
|
|
Excellent info guy...I don't seem to have added too much NaOH since the drainwater is yellow for some reason (probably iron (III) hydroxide on a
colloidial level).
I'd go the brute force 12AX7 way, but other than cans, I don't have any decent crucibles and my only good heat source is a large torch that runs on
disposable tanks (ow my wallet) and isn't very easy to control the temp with.
Anyone trying this should realize that it has to be electrolyzed into the acid. I left a small piece in ~60% sulfuric overnight and not a bit of it
dissolved. Not even H2O2 mixed into the acid could attack it (I used this mix to rip up some US nickels much faster than just sulfuric acid could ever
accomplish).
[Edited on 4-23-07 by UnintentionalChaos]
Department of Redundancy Department - Now with paperwork!
'In organic synthesis, we call decomposition products "crap", however this is not a IUPAC approved nomenclature.' -Nicodem
|
|
12AX7
Post Harlot
Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline
Mood: informative
|
|
I've got a hunk of horribly badly pitted stainless bar due to leaving it sit in concentrated HCl for weeks.
I don't think H2SO4 forms much of a complex, but HCl does, which is likely the reason the Cr2O3 passivation layer on the metal has given us two
different results for these two acids.
Tim
[Edited on 4-24-2007 by 12AX7]
|
|
guy
National Hazard
Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline
Mood: Catalytic!
|
|
Quote: | Originally posted by 12AX7
I've got a hunk of horribly badly pitted stainless bar due to leaving it sit in concentrated HCl for weeks.
I don't think H2SO4 forms much of a complex, but HCl does, which is likely the reason the Cr2O3 passivation layer on the metal has given us two
different results for these two acids.
Tim
[Edited on 4-24-2007 by 12AX7] |
so HCl works?
|
|
woelen
Super Administrator
Posts: 7987
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
HCl + H2O2 definitely works. HCl alone is VERY slow.
|
|
guy
National Hazard
Posts: 982
Registered: 14-4-2004
Location: California, USA
Member Is Offline
Mood: Catalytic!
|
|
So any update on the separation?
|
|
Pyridinium
Hazard to Others
Posts: 258
Registered: 18-5-2005
Location: USA
Member Is Offline
Mood: cupric
|
|
I think your strategy sounds good, keep air bubbling into the solution to speed the rusting-out of the Fe. Keep the pH high with excess NaOH so the
Cr hydroxo complex stays in solution.
Sounds like it should work just fine.
|
|