Urushibara Catalysts
Does the Urushibara reduce imine?
[Edited on 16-7-2006 by Filemon]
|
|
solo
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3973
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline
Mood: ....getting old and drowning in a sea of knowledge
|
|
This is some information which may be of use.........solo
http://designer-drugs.com/pte/12.162.180.114/dcd/chemistry/u...
It's better to die on your feet, than live on your knees....Emiliano Zapata.
|
|
flyingbanana
Harmless
Posts: 38
Registered: 1-3-2005
Member Is Offline
Mood: No Mood
|
|
I've never been able to get this catalyst to work...I think it is very picky to the quality of your reagents and the preparation. I even have a copy
of the original book where that article is from
|
|
not_important
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Think they should have given you this link
http://designer-drugs.com/pte/12.162.180.114/dcd/chemistry/r...
Urushibara cats work, just need to note the limitations, similar to Raney. They tend to be more forgiving of reagent quality than Raney, but there are
limits.
|
|