Author: Subject: Mercury electrodes?
Sir_Gawain
Hazard to Others
***




Posts: 493
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline

Mood: Still in 2022

[*] posted on 7-12-2024 at 14:08
Mercury electrodes?


Would a mercury electrode be inert enough to run a chlorate cell? I know one problem might be the absorption of elemental sodium by the mercury, but would that negatively affect the production of chlorate?



“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
View user's profile Visit user's homepage View All Posts By User
Cendre
Harmless
*




Posts: 33
Registered: 1-12-2023
Location: California/France
Member Is Offline

Mood: Carbonated

[*] posted on 9-12-2024 at 22:47


How would you even use that? You would need your wires to go deep in solution and then if mercury was used to substitute another material you would still get possible contamination from copper or whatever material used to conduct current. Also mercury additionally to being toxic, especially when airborne (electricity will get your solution hot, bad idea), has a tendency to amalgam. All in all unless it really has a special case in your cell I don’t think it is worth the trouble or hazard.

As for chlorate cells, platinum electrodes are the best of course, MMO give decent results, lead dioxide are supposed to work (I personally got a hefty amount of lead precipitation but my lead dioxide was homemade and badly made) and lastly good old graphite which will be eaten through and give some carbon contamination but it can be kept to a pretty small amounts. All in all, it mostly depends on your use of chlorate and purity and speed of reaction needed.
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8082
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 10-12-2024 at 01:52


No, mercury is not suitable as anode material. It will be oxidized, most likely to the +2 oxidation state. No chlorate will be formed, nor chlorine. At a mercury cathode you will get hydrogen and hydroxide in solution, but that also can be done with nearly any other metal.

So, forget using mercury electrodes for electrolysis. You'll get a horribly toxic mess, which you don't want to have around.

[Edited on 10-12-24 by woelen]




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User