Chromate/dichromate from stainless steel via oxalic acid route


Finally after a long research time got potassium chromate / dichromate from stainless steel (SS) in a more or less pure form.

I tried the SS + HCl, hydroxide(or carbonate), oxidize, cristallization, but got no good resutls, because a lot of another salt always was interfering/cristallizing. (mainly from the HCl + Hydroxide or oxidation with Na/K hypochlorite.)

Tried different oxidizers, H2O2, potassium persulfate, Na/K hypochlorite.

So in order to minimize adding other cations and removing other metals from the solution , the best route I found was to use oxalic acid.

Chromium oxalate is soluble in oxalic acid as long as Ph is less than 2., which by using a 1M oxalic acid this requirement is met.
Fe (II) oxalate is almost insoluble (0.097 g/100ml (25 °C))
Fe (III) oxalate is soluble, but as oxalic acid is a reducing agent, any Fe (III) is reduced to Fe(II)
Ni oxalate is also insoluble (if SS contained nickel).

this is the procedure:

1) MAKING CHROMIUM OXALATE:

Dissolve SS in 1M Oxalic acid (this procees takes long time)
I used 1 or 2 molar oxalic acid, but any concentration which gives you Ph 1 or less is ok. The stronger the oxalic acid the faster the dissolution.
Use heat (I used boiling reflux) for speeding things.
Use stirrer (because Fe(II) oxalate deposites in the SS) but if the SS is magnetic, the stirrer is of no use, but using the stirring magnet slow, the slow magnetic field shakes the SS)
as an example: 3 SS sponges (aprox 30gr) took 500 ml 2 M oxalic acid and 6 hrs to fully dissolve. (it was an big excess, but I wanted to reduce the time as much as possible.)
Excess oxalic acid is bad for the second part (removing the oxalate)

Filter by decantation (because filtering Fe(II) oxalate is very difficult- or at least for me. the longer the decantation the better (I use 24 hs)
You will obtain a strong violet solution (Cr oxalate) and a precipitate of the other metals of the SS - mainly Fe(II) oxalate.

2) REMOVING THE OXALATE - MAKING CHROMIUM HYDROXIDE:
To the Cr oxalate solution add Ca(OH)2 by drops till the Ph of the solution reaches 5-6. (try not to add an excess because it will start precipitating the Chromium hydroxide, which starts to precipitate at ph 5-6)
You can more or less eyeballin when adding the Ca(OH)2 does not produce a lot of precipitate.
Also some leftover Iron that was in solution will precipitate as Iron hydroxide once you reach ph 4+, thus cleaning your new Cr(OH)3 solution.

Filter by decantation the Cr(OH)3 from the Ca oxalate.
(you will be left with a green/blue solution -when looked with a light behind or blue/red by reflecting light)

If you use an excess of oxalic acid, you will need a lot of Calcium hydroxide.

3) MAKING THE "SALT" CHROMATE BY ADDING HYDROXIDE + OXIDIZING THE CHROMIUM HYDROXIDE
Add "salt" hydroxide to get the ph of the chromium hydroxide solution to ph 10+ (dark blue ph paper). By "salt" I mean , KOH, NaOH, CaOH, depending which chromate do you want. (maybe ammonia could also be used if you need NH4 chromate - did not tried this, but why not.)

Oxidize by adding H2O2. Do not add to much, heat slowly, for example till 50C, and it has an induction time of aprox 10 minutes. (This is very important, because you think nothing is happening, and you add an excess, and the suddenly you have overflowing bubbling chromate solution everywhere....)
I add a few drops (3-4) 10% H2O2 to 50 mls Chromium hydroxide solution.
After aprox 8-10 minutes, the solution goes from green/blue to yellow.
Boil it to remove excess H2O2.
Let it decant, for removing, if any Iron was left, because it precipitates as a red flocculent precipitate.- very minor.

In the end you will be left with a strong yellow solution of your chromate that could be reduced (the liquid) by heat till cristalls appear or till dryness.
(depending on the purity you want)

If you want the dichromate, add H2SO4 to acidify. (tried HCl, but H2SO4 is better)

Test:
Add lead acetate (or any soluble lead solution) to a solution of the chromate -> yellow lead chromate precipitates

Add acid (H2SO4 better) to chromate -> change from yellow to orange red







Go SAFE, because stupidity and bad Luck exist.
View user's profile View All Posts By User
Keras
International Hazard
*****




Posts: 1018
Registered: 20-8-2018
Location: (48, 2)
Member Is Online


[*] posted on 21-11-2024 at 23:09


This is a good way, but I think it’s a bit of an overkill. Dissolving stainless steel in HCl, then turning the solution alkaline will precipitate hydroxides of chromium, iron and nickel. Adding an oxidant, such as hydrogen peroxide or bleach, will oxidise all those ions into Cr VI, Fe III (Ni won’t oxidise, I think), the only one soluble is Cr VI. Further operations of rinsing and turning the pH to neutral will get you rid of the iron.

This is quite detailed in this video (in French) where the guy obtains quite pure calcium chromate from stainless steel cutlery (his stainless steel is 18/0, no nickel) and egg shells.

[Edited on 22-11-2024 by Keras]
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 602
Registered: 15-1-2024
Location: Home
Member Is Offline

Mood: British

thumbup.gif posted on 22-11-2024 at 05:19


The chromium salt with undefined color is an oxalate complex. I have some in a test tube (I'm still thinking what to do with it and what color is that). The bubbles were mostly carbon dioxide from oxidation of oxalate.

I would prefer to precipitate oxalate as a calcium or copper salt (calcium seems better, thanks for testing), decant and then add a base and oxidiser but, as you used peroxide, the only residues are water and carbon dioxide. And you solved two problems (disposal and removal of the anion) at the same time.

Well done.




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User

  Go To Top