Author: Subject: Attempt to make magnesium chromate
Lion850
National Hazard
****




Posts: 517
Registered: 7-10-2019
Location: Australia
Member Is Offline

Mood: Great

[*] posted on 18-9-2021 at 20:50
Attempt to make magnesium chromate


I thought a colored magnesium salt would be cool, and was keen to do something with my chromium trioxide so decided to give magnesium chromate a go. Looking online most references mentions MgCrO4 as being yellow, but sometimes orange or orange brown. An image search brings up yellow, orange, and orange-brown photos. And there are photos that shows magnesium dichromate as yellow! I don't think some of the photos from Indian supplier websites is completely accurate.

From reading articles online it is clear that both magnesium chromate and dichromate exists in various hydrates, the pentahydrate being the most common from what I can gather. The higher hydrates usually loose some water under 100C, the pentahydrate is stable until well over 100C, and the compounds themselves don't decompose until several 100C. So it seemed feasible to dry the salt on a steambath.

My starting materials were CrO3 and MgO. Both old chemicals, with the CrO3 being slightly damp and the MgO seemingly to have partially converted to carbonate; see below. For the stoichiometry I simply assumed pure chemicals.
1.jpg - 587kB

- 20g CrO3 added to a small beaker with 30g water, this was then stirred until fully desolved.
- 8.1g of MgO was measured out (it's fluffy and a large bulk) and slowly added to the CrO3 solution while stirring. With each addition there was a bit of bubbling, and the solution got quite hot.
2.jpg - 624kB

- The bubbling confused me and I then wondered whether some MgO had reacted with CO2 and converted to the carbonate. To test this I added some of the MgO to hydrochloric acid; and it did indeed bubble a tiny bit but much less than a pure carbonate would. So I assume the MgO did contain carbonate but not a lot.
- By the time all the MgO was added the color of the solution was red-brown and it was not far from boiling.
- I left it to stir for 2 hours. By then we was still a few tiny flakes of MgO going around and the pH was around 4; which indicated to me that most of the chromium acid had reacted.
- The solution was then left to gravity filter overnight. The next morning this wine red filtrate was observed.
3.jpg - 304kB

- There was a small amount of what I assume is MgO in the remainder, but note the layer of black particles on the filter paper. Can this be metallic chromium, and if so why?
4.jpg - 393kB

- The filtrate was then put on a steam bath. After 2 hours a few grams of weight was lost and there was a crust on the liquid.
5.jpg - 569kB

- More weight was lost the next 2 hours, but very little, and then nearly nothing during a final 2 hours. Then it looked like this.
6.jpg - 402kB

- I realized the steam bath was not going to dry this any more, but I also wondered whether the salt dissolved in its own water of crystallization. The evaporating dish was left on the bench while I had to do something else.
- When I returned 2 hours later it was solid!
7.jpg - 470kB

- It was quite dry, with a consistency of a cake of soap: The spatula struggled to penetrate it but little shavings could be scraped off. Below shows the bigger broken up pieces with a lot of shavings already removed.
8.jpg - 656kB

- The final recovery was 33.3g. The thin shaving are more orange-yellow, but the bulky pieces have a more orange-brown outside layer.
9.jpg - 392kB

So what is it? The chromate or dichromate? From the color it appears it may be a mix of the two, although the below equation matches the obtained product weight perfectly:

MgO + 2CrO3 + 5H2O = Cr2MgO7.5H2O

Of course there is now way I can get 100% yield because some bit were still left in the evaporating dish, it may not be 100% dry, could be a mix of hydrates. So I am still inclined to think it is a mix of chromate and dichromate. Your comments and thoughts will be appreciated!

I did a few very basic tests:
- I drop methanol onto a tiny bit of the product. When methanol is dropped onto my CrO3 starting material it immediately catches fire (quite spectacular) but when dropped onto the product there is no reaction.
- I poured some concentrated HCl into the evaporating dish that still had some scraps of product; the product goes dark and then green and dissolves in the acid with a smell of chlorine.
10.jpg - 421kB
View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1682
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 19-9-2021 at 02:25


colorful chemicals should always come with a taste-rating.



~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5135
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 19-9-2021 at 05:14


The dark stuff on the filter is probably something like Chromium (III) chromate (VI)
An interesting outcome would be
https://en.wikipedia.org/wiki/Chromium(IV)_oxide

Wash it with plenty of water, then se if it is magnetic.



[Edited on 19-9-21 by unionised]
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8082
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 19-9-2021 at 11:46


I have reagent grade magnsium chromate. It has a golden yellow color and is quite soluble in water. It certainly is not as orange as the material you end up with. I have the impression that your product is a mix of the chromate and dichromate.



The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
chloric1
International Hazard
*****




Posts: 1159
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 7-11-2024 at 19:06
pH too low


Pretty sure you mentioned a pH of 4.1. The dichromate ion begins to form at pH of 3-4. I’d think you need to raise pH at least to 6 to have all chromate, maybe even a pH beyond 7.



Fellow molecular manipulator
View user's profile View All Posts By User
Admagistr
Hazard to Others
***




Posts: 383
Registered: 4-11-2021
Location: Central Europe
Member Is Offline

Mood: The dreaming alchemist

[*] posted on 7-11-2024 at 20:30


I once made MgCrO4 from MgO, distilled water and CrO3, it was yellow! Definitely not orange! And the MgO dissolved well, no problem, the problem came later when I boiled it to force it to crystallize, with a water droplet trap, it was a ground glass part, there was an accident, an explosion due to the overpressure of the water vapour and the chromate splashed all over the room, then I wiped the toxic droplets all over the room and there was always another yellow spot...Thus the unpleasant ending and I lost all the yield...
View user's profile View All Posts By User

  Go To Top