Maui3
Harmless
Posts: 20
Registered: 9-9-2024
Member Is Offline
|
|
Nitrocellulose won't ignite..
My nitrocellulose just gets burnt.. I tested the normal cotton too, and this burned quite nicely. I am quite new to energetics, so this might be
stupid question, but could it have something to do with the pH being too low or high? I think my nitrocellulose was still quite acidic, even after the
washings.. Also, my nitrate salt didn't dissolve in all the sulfruic acid, so there is some nitrate salt of the outside of the cotton, which even
after scraping off, still doesn't make the cotton ignite..
|
|
Keras
National Hazard
Posts: 879
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline
|
|
I hope this is not your last post… :/
|
|
fx-991ex
Hazard to Self
Posts: 97
Registered: 20-5-2023
Member Is Offline
|
|
Make sure to clean residue correctly, use medium/warm water and work it more.
Also make sure its very completely dry before testing.
|
|
Maui3
Harmless
Posts: 20
Registered: 9-9-2024
Member Is Offline
|
|
Haha! Definitely not my last pos-
.. Thank you fx-991ex for the tips.. Will try!
|
|
Sturge11
Harmless
Posts: 18
Registered: 4-9-2019
Member Is Offline
|
|
Metallica said it best. GASOLINE!
|
|
Laboratory of Liptakov
International Hazard
Posts: 1382
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
Your nitrocellulose is not dry. The looks a like dry between fingers, but isnt. There is about 10 - 15 % water. You set hot airgun on 50 Celsia on 30
minute for 1g NC distance 5 cm.....
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
Sir_Gawain
Hazard to Others
Posts: 402
Registered: 12-10-2022
Location: Due South of Due West
Member Is Offline
Mood: Like a pendulum
|
|
Could you post some pictures? That might help.
The nitrate salt should dissolve completely. Which nitrate is it?
“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
|
|