Soda lime glass tubing - local seller
Does anyone know of a place you can buy soda lime glass tubing locally? I don't want to wait for shipping if I can avoid it.
Yeah, I can setup my jointed distillation kit, but for tiny experiments it's nice to just bend a glass tube and fit it into a test tube. I found some
sources online, but the price seems high or the shipping delays seem significant so I'm hoping to find it locally.
Thanks!
|
|
esquizete_electrolysis
Harmless
Posts: 13
Registered: 9-10-2018
Location: N.C. RT
Member Is Offline
|
|
It may be possible to find some glass tubing sold as reusable straws, but these are often borosilicate. If there are any glassblowing studios near
you, it would probably be worth while speaking to them.
|
|
Sir_Gawain
Hazard to Others
Posts: 462
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline
Mood: Stable
|
|
I’ve made ampoules with glass straws before, and they worked great.
[Edited on 8-25-2024 by Sir_Gawain]
“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
|
|
bnull
Hazard to Others
Posts: 484
Registered: 15-1-2024
Location: South of the border, wherever the border is.
Member Is Offline
Mood: Happy New Year!
|
|
Some art stores have glass tubing for, well, art.
Quod scripsi, scripsi.
B. N. Ull
P.S.: Did you know that we have a Library?
|
|
inanium
Harmless
Posts: 14
Registered: 1-12-2020
Member Is Offline
|
|
Thanks for the replies.
I contacted my local sci/chem supplier and they used to carry lime glass tubing but stopped because every shipment arrived broken.
I ended up ordering some borosilicate glass drinking straws off Amazon for about $6. There's a video from Cody's Lab where he melts borosilicate with
a MAPP torch, which I have, so I think it will work. I'm only trying to make a single bend in the tube for a simple distillation setup using a test
tube.
|
|
Sir_Gawain
Hazard to Others
Posts: 462
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline
Mood: Stable
|
|
I’m pretty sure the straws I used to make ampoules were borosilicate, and they softened easily with a propane torch.
“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
|
|
Sulaiman
International Hazard
Posts: 3734
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
Quote: Originally posted by inanium | ... I'm only trying to make a single bend in the tube for a simple distillation setup using a test tube. | I
can, with patience, bend a borosilicate tube
or melt the end just enough to soften the edges of a cut end,
using a domestic butane gas cooker.
A MAPP gas torch should be more than hot enough.
-
Making a bend is easy, getting it 'nice-looking' needs luck or practice.
-
Keep in mind, non-glowing glass can still be hot enough to BBQ skin
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Morgan
International Hazard
Posts: 1705
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
A "soda" straw
https://thecraftybartender.com/products/strawhopper-recyclab...
[Edited on 27-8-2024 by Morgan]
|
|
Dr.Bob
International Hazard
Posts: 2759
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: Mildly disgruntled scientist
|
|
inanium,
Where are you located? You asked about local sources, but that depends on where local is. As a note, I can get short pieces of glass tubing from
some scraps I have if anyone in the US wants some. Various pipettes also can be used as glass tubing, from Pasteur pipettes to volumetric ones.
Bob
|
|
inanium
Harmless
Posts: 14
Registered: 1-12-2020
Member Is Offline
|
|
Located in Southern California for now.
I guess I should look into a proper glassblowing setup. It would be nice to make test tubes and other things from basic glass tubing. It's hard to
find time though. Every time I find something else to DIY, it just cannibalizes the time I have to do the thing I'm actually trying to accomplish.
|
|
fx-991ex
Hazard to Others
Posts: 102
Registered: 20-5-2023
Member Is Offline
|
|
Yes you can work small borosilicate tubes with a simple propane torch or MAPP torch for bigger thicker tubes(12mm/2mm thick).
|
|