Author: Subject: Refining mercury from cinnabar
Mailinmypocket
International Hazard
*****




Posts: 1351
Registered: 12-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 6-1-2015 at 08:08


This is the closest that YouTube (aka chemistry school for some) was able to find:

http://youtu.be/znQh7m2mkiQ
View user's profile View All Posts By User
Texium
Administrator
Thread Untopped
22-12-2015 at 07:41
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 10-5-2018 at 12:37


Is cinnabar rly that expensive?!



View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4666
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Preparing to defend myself (academically)

[*] posted on 10-5-2018 at 12:45


Is it rly necessary to bump a lot of old threads that have been inactive for years with useless one liners that add nothing interesting to the discussion?




Answer: no




Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
Johnny Windchimes
Hazard to Self
**




Posts: 61
Registered: 28-5-2019
Member Is Offline

Mood: Sorry, it's my chimes~!

[*] posted on 8-10-2020 at 15:32


My turn....

I looked through the whole thread and didn't see this electro process mentioned, so here it is:

I have successfully done this several times. First with 50 grams of Cinnabar from eBay, all the way up to 2 kilograms (stuff is 8.1 g/cm3; dense!).

Get yourself a 2 amp / 20 volt DC power supply and you're off!

My recommendations:

-Use two platinum electrodes. Needs to be made of something that both wont dissolve in the electrolyte, nor amalgamate with the elemental Hg.

-PURE tungsten welding electrodes are also a great choice, as tungsten does not form amalgams either. I have not personally used tungsten but if I do this again I shall try them. Try automotive supply and welding shops.

-CAREFULLY powderize (as best you can) the cinnabar. This can make dust thats obviously super bad to breath and bad in general to spread around. Mortar and pestle make a HUGE cloud in my experience; I used a small coffee grinder but that makes even smaller airborne "smoke" almost size dust particles when its opened.....

-Once its (cinnabar powder) in the mix of NaOH and sulphide, give it LOTS of time to dissolve into solution. Lots of stirring. After it has (or as much has dissolved as is going to), filter it with a coffee filter and a funnel. If you don't, the junk left over (impurities in the cinnabar, etc) can amalgamate with the newly formed Hg metal, and it just makes for a cleaner prep.

-Use a secondary containment device. I put the entire electro setup into a nice and big ol' plastic bin in case any spills happened.


Enjoy, because it does work!




Attachment: US1718103 - Cinnabar electrolysis to Hg - Copy.pdf (213kB)
This file has been downloaded 423 times Stoichiometry Calculations for Hg Metal via Electrolysis of HgS (Cinnabar) - Copy.png - 60kB

[Edited on 8-10-2020 by Johnny Windchimes]




~Incredibly profound and/or wise quote goes here~
View user's profile View All Posts By User
monolithic
Hazard to Others
***




Posts: 436
Registered: 5-3-2018
Member Is Offline

Mood: No Mood

[*] posted on 9-10-2020 at 13:48


Quote: Originally posted by Mailinmypocket  
This is the closest that YouTube (aka chemistry school for some) was able to find:

http://youtu.be/znQh7m2mkiQ


Very old post but can someone explain how this works? I'm just starting to read on this process but it seems it has to run at very high temperatures... but glass can't withstand 600C+?
View user's profile View All Posts By User
Catslovechemistytoo
Harmless
*




Posts: 17
Registered: 15-7-2024
Member Is Offline


[*] posted on 8-9-2024 at 09:15


Quote: Originally posted by Johnny Windchimes  
My turn....
Get yourself a 2 amp / 20 volt DC power supply and you're off!

My recommendations:

-Use two platinum electrodes. Needs to be made of something that both wont dissolve in the electrolyte, nor amalgamate with the elemental Hg.

-PURE tungsten welding electrodes are also a great choice, as tungsten does not form amalgams either. I have not personally used tungsten but if I do this again I shall try them. Try automotive supply and welding shops.

Enjoy, because it does work!


Can titanium electrodes be used instead?

And where to get the Na2S? Can H2S just be bubbled through NaOH solution?

Or can we just dissolve sulfur in NaOH and then use this sulfides solution instead of pure Na2S?

[Edited on 8-9-2024 by Catslovechemistytoo]

[Edited on 8-9-2024 by Catslovechemistytoo]
View user's profile View All Posts By User
Precipitates
Hazard to Others
***




Posts: 156
Registered: 4-12-2023
Location: SE Asia
Member Is Offline

Mood: Acid hungry

[*] posted on 8-9-2024 at 19:00


Quote: Originally posted by Catslovechemistytoo  

Can titanium electrodes be used instead?



I'm not sure of the corrosion of titanium under these conditions - it's resistant at low temperatures, but starts to amalgamate at much higher temperatures. It's labelled as having just "good" compatibility:

Compatibility of Titanium and Mercury

Quote: Originally posted by Catslovechemistytoo  


And where to get the Na2S? Can H2S just be bubbled through NaOH solution?

Or can we just dissolve sulfur in NaOH and then use this sulfides solution instead of pure Na2S?


I would probably try the following patent's method to produce a NaOH and sodium sulphide solution:

Manufacture of sodium sulfide and sulfite

...as mentioned in this previous thread:

Sodium sulphite and sulphide from sulphur and NaOH

Be very careful working with mercury and its compounds - secondary containment is essential.
View user's profile View All Posts By User
Catslovechemistytoo
Harmless
*




Posts: 17
Registered: 15-7-2024
Member Is Offline


[*] posted on 11-9-2024 at 02:38


Quote: Originally posted by Precipitates  

I'm not sure of the corrosion of titanium under these conditions - it's resistant at low temperatures, but starts to amalgamate at much higher temperatures. It's labelled as having just "good" compatibility:

Compatibility of Titanium and Mercury

Quote: Originally posted by Catslovechemistytoo  


And where to get the Na2S? Can H2S just be bubbled through NaOH solution?

Or can we just dissolve sulfur in NaOH and then use this sulfides solution instead of pure Na2S?


I would probably try the following patent's method to produce a NaOH and sodium sulphide solution:

Manufacture of sodium sulfide and sulfite

...as mentioned in this previous thread:

Sodium sulphite and sulphide from sulphur and NaOH

Be very careful working with mercury and its compounds - secondary containment is essential.


Okay, thank you for your answer. So Titanium should be fine at these temperatures. I think I'll just dissolve sulfur in NaOH solution and try dissolving HgS in it. As for electrolysis - how do I know when to stop it? My guess is that when H2 or whatever else starts evolving at cathode besides mercury then it's time to stop.
Can this be done inside of a plastic container(PP or HDPE)? I don't have large borosilicate beakers and doing this in regular glass is risky because it can crack.
View user's profile View All Posts By User
Precipitates
Hazard to Others
***




Posts: 156
Registered: 4-12-2023
Location: SE Asia
Member Is Offline

Mood: Acid hungry

[*] posted on 11-9-2024 at 17:57


When mercury stops being produced.

HDPE should be okay.
View user's profile View All Posts By User