Why not use a PbO2 anode if making sulfuric acid?
One can easily make one from a bit of lead, check YT videos, there are examples many showing this procedure.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6342
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 15-7-2024 at 02:19


Quote: Originally posted by Mateo_swe  
Seems to be a really old thread.

Why not use a PbO2 anode if making sulfuric acid?
One can easily make one from a bit of lead, check YT videos, there are examples many showing this procedure.

Or even easier. Use a lead anode. After a short amount of use it obtains a PbO2 coating. And then you have a nice PbO2 anode.