I use a base bath frequently for glassware, it does not hurt it or bother the joints. The amount of glass removed is atoms thick, not measurable.
Only a very long time (days to months) there will ever remove enough glass to matter. HF on the other hand will etch glass in a few hours, and it
does not ever look the same again. I have a few flasks that HF was a byproduct in, and they all look bad when wet, and worse when dry. They look
sand blasted or such.
Scotch bright pads are good for cleaning the joints if they get dirty. The rubber septa will sometimes leave a film of goo on them, especially after
exposure to acid.
|
|
Sir_Gawain
Hazard to Others
 
Posts: 487
Registered: 12-10-2022
Location: [REDACTED]
Member Is Offline
Mood: Still in 2022
|
|
Can anyone with some geology experience verify if this is actually cinnabar? https://www.etsy.com/listing/1705692311/australian-rough-cin...
“Alchemy is trying to turn things yellow; chemistry is trying to avoid things turning yellow.” -Tom deP.
|
|
Rainwater
National Hazard
  
Posts: 982
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
Distill a sample at 600c. Not efficient but its worked for 10⁴ years
"You can't do that" - challenge accepted
|
|
yobbo II
National Hazard
  
Posts: 769
Registered: 28-3-2016
Member Is Offline
Mood: No Mood
|
|
How can the Alpha and the Beta CaSO4:0.5H20 have different solubilities (in the long term)?
Perhaps the study did not wait for days/weeks for all to dissolve, ie. the Beta is slower???
Yob
|
|
4-Stroke
Hazard to Self

Posts: 59
Registered: 20-4-2024
Location: Canada
Member Is Offline
Mood: Often Wrong, Never Unsure
|
|
Sulfur Chlorides Using HCl instead of Chlorine
I know this might be a dumb question, but I was wondering if HCl gas (which is easier and cheaper to prepare than chlorine) could be used instead of
chlorine in the synthesis of sulfur chlorides? Thanks.
Ukrainium
|
|
Pages:
1
..
102
103
104 |