Growing quasicrystals at home?
There are several stoichiometric formulas of alloys that can form quasicrystals.
Would it be possible, using a melting furnace and some thermally insulating container that cools the alloy very slowly, to manufacture and grow
macroscopic-sized quasicrystals (visible to the naked eye) at home?
[Edited on 14-5-2024 by angeltxilon]
|
|
Precipitates
Hazard to Others
 
Posts: 154
Registered: 4-12-2023
Location: SE Asia
Member Is Offline
Mood: Acid hungry
|
|
Potentially, depending on your set-up.
In this paper, macroscopic quasicrystals, the authors were able to produce dendrites of 3 mm size (probably just about visible to the naked eye) from an
aluminium, copper and lithium (Al6CuLi3) mix heated to 850°C. They mentioned that the size of the crystals may have been
improved if a larger container had been used to cast the alloy.
|
|
Rainwater
National Hazard
  
Posts: 987
Registered: 22-12-2021
Member Is Offline
Mood: Break'n glass & kick'n a's
|
|
What type of time scall is required here? Hours, days?
crucible are consumable equipment, controlled atmosphere will prolong their usage, but not indeffentetly.
Edit. Read the paper.
5 hours to > 2 months.
I think the quenching may be a factor. Slower crystallization, bigger crystals
Finding a container that can hold molten lithium for 5 hours, thats a challange on a budget
[Edited on 14-5-2024 by Rainwater]
"You can't do that" - challenge accepted
|
|
angeltxilon
Harmless
Posts: 21
Registered: 24-10-2015
Member Is Offline
Mood: No Mood
|
|
I wonder if there are more manageable alloys that do not require a controlled atmosphere (no reactive metals like lithium, or volatile metals like
zinc).
I am especially interested in those that could crystallize into dodecahedra and similar polyhedra.
[Edited on 15-5-2024 by angeltxilon]
|
|
Precipitates
Hazard to Others
 
Posts: 154
Registered: 4-12-2023
Location: SE Asia
Member Is Offline
Mood: Acid hungry
|
|
There are such beautiful crystals in this paper, high-temperature solution growth of intermetallic single crystals and quasicrystals, and, according to the authors:
"Growth of single crystals from metallic solutions requires very simple equipment: box and vertical tube furnaces, a glass bench for evacuating and
sealing quartz tubes, crucible materials and, in some cases, an arc melter for pre-alloying elements and for working with Ta."
|
|
Morgan
International Hazard
   
Posts: 1730
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
I liked this one a lot.
https://en.wikipedia.org/wiki/Holmium%E2%80%93magnesium%E2%8...
|
|
Precipitates
Hazard to Others
 
Posts: 154
Registered: 4-12-2023
Location: SE Asia
Member Is Offline
Mood: Acid hungry
|
|
I just wish it was a cm as oppose to mm grid!
The pessimist in me will say though - can't we just take any metal, cast it into a mould with that shape, and achieve the same (but bigger) result?

As indeed we've been doing since Roman times:
https://en.wikipedia.org/wiki/Roman_dodecahedron
As evidenced by the rather alien dodecahedra that have been found.
But I realise that's probably not the point.
|
|