[*] posted on 24-12-2023 at 17:55
Zircon mineral processing,Zr,Hf,Th separation.


I have obtained sand from ground Zircon mineral,it is used in metal casting in a foundry,it is very cheap and available in 25 kg bags.I would like to separate Zr,Hf and Th compounds from it. The sample shows a higher radioactivity due to the Thorium content,which is related to Zirconium and Hafnium.It is clear to me that I have to start by dry melting it with alkaline hydroxide,but separating the very close Hf from Zr will probably be a difficult task in more modest conditions. I have read that one can use some complexes I think using KSCN.Has anyone attempted something similar under home chemist conditions?Getting hafnium compounds,which is expensive and zircon contains more than 4% of it is an interesting possibility.Also separating Th compounds would be useful,so that thorium interfere via its radiation action with zirconium minerals and compounds and damages natural mineral zircon structurally and breaks its crystal lattice into amorphous form over millions of years.
View user's profile View All Posts By User
Fery
International Hazard
*****




Posts: 1026
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline


[*] posted on 25-12-2023 at 04:23


Just guessing, but cannot it be dissolved in an acid (very likely hot conc. H2SO4) or acid mixture (like HF+HNO3) and separated electrolytically due to differences in redox potential?
Here they facilitated the dissolution by milling ZrSiO4 with Al2O3:
https://sci-hub.ee/10.1016/0254-0584(94)01459-T
View user's profile Visit user's homepage View All Posts By User
Stokes
Harmless
*




Posts: 7
Registered: 6-11-2023
Member Is Offline


[*] posted on 25-12-2023 at 05:28


It is quite difficult to separate zirconium and hafnium, even industrially, and they have very similar chemical properties. Unless you're wanting to do this for the interest, it probably isn't worth it to separate the two, particularly since a small amount of hafnium won't make any difference for most reactions. If you're wanting to try, this patent is the simplest method I've seen that ought to give good yields, though it certainly isn't easy unless you have plenty of sodium.
View user's profile View All Posts By User
Admagistr
Hazard to Others
***




Posts: 375
Registered: 4-11-2021
Location: Central Europe
Member Is Offline

Mood: The dreaming alchemist

[*] posted on 25-12-2023 at 07:54


Thanks a lot for the advice! The concentrated H2SO4 looks good,I'll try it,possibly melting with KHSO4 might help,as it is done when we want to dissolve corundum.SiO2 is separated and we are left with zirconium,hafnium,Th salt.Zirconium contains lanthanides,its chemical composition is interesting and varied in terms of impurities. I'll study the patent,let you know and send photos when I try it.I've always been attracted to hafnium compounds because of their affinity to zirconium,Zr makes up many gems and Hf does too,but in some ways they have slightly different properties and that's what attracts me;-)