[*] posted on 11-12-2023 at 02:11
Fake Terbium?


Hello everybody, some time ago I purchased a 10g sample of "terbium" from eBay.
Now I dissolved in HCl, but it does not seems like Terbium at all. There is no trace of green fluorescence. At the beginning I thought it could have been quenched by water, but there is no way to see the green fluorescence even with the dry product.
Precipitating the tungstate gives a slightly pink fluorescence(?).
I don't know what it could be, maybe some cheaper rare earth?
It appears to not be fluorescent at all!

Now I precipitated with NaOH and kept the Hydroxide (white powder)
It could be possible that the fluorescence is somehow quenched by water? I think it should be visible in minimum amount.

here is a photo of it and a photo of a real terbium solution I got previously.



2.JPG - 932kB1.JPG - 1.5MB
View user's profile View All Posts By User
Maurice VD 37
Hazard to Self
**




Posts: 67
Registered: 31-12-2018
Member Is Offline


[*] posted on 11-12-2023 at 02:41


Why don't you first weigh a bit and dissolve it in HCl, then evaporate the solution. Or precipitate the solution with NaOH, or with another reactant, then filtrate and weigh the precipitate ? Comparing the weights should give you an information.
View user's profile View All Posts By User
ItalianChemist
Hazard to Others
***




Posts: 180
Registered: 26-1-2011
Location: Italy
Member Is Offline

Mood: No Mood

[*] posted on 11-12-2023 at 02:46


Quote: Originally posted by Maurice VD 37  
Why don't you first weigh a bit and dissolve it in HCl, then evaporate the solution. Or precipitate the solution with NaOH, or with another reactant, then filtrate and weigh the precipitate ? Comparing the weights should give you an information.

I already recovered the precipitate.
Unfortunately I don't know if I lost some product during the filtration, so I don't know if it would work!
The metal could have a slightly lower atomic weight, because it didn't fully dissolve in the acid!



[Edited on 11-12-2023 by ItalianChemist]
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1251
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 11-12-2023 at 04:11


Iron contamination is usually big problem in fluorescent materials. Tb(III) is very slightly pink, so don't expect to observe some strong coloration of its compounds. If you add NaOH and persulfate in to your Tb(III) solution and heat it, you should obtain black precipitate of terbium(III, IV) oxide Tb4O7. Only preseodymium give you similarly looking product (but Pr(III) is green solution, so you cannot mistake it for Tb(III)).
View user's profile View All Posts By User
ItalianChemist
Hazard to Others
***




Posts: 180
Registered: 26-1-2011
Location: Italy
Member Is Offline

Mood: No Mood

[*] posted on 11-12-2023 at 04:22


Quote: Originally posted by Bedlasky  
Iron contamination is usually big problem in fluorescent materials. Tb(III) is very slightly pink, so don't expect to observe some strong coloration of its compounds. If you add NaOH and persulfate in to your Tb(III) solution and heat it, you should obtain black precipitate of terbium(III, IV) oxide Tb4O7. Only preseodymium give you similarly looking product (but Pr(III) is green solution, so you cannot mistake it for Tb(III)).

Tb salt are white, but they have very strong green fluorescence.
I already have some small sample of terbium compound. They have most intense fluorescence I have ever seen.
With NaOH only the hydrated hydroxide seems to precipitate.
I will test for iron presence, but I don't think it is the case.



[Edited on 11-12-2023 by ItalianChemist]
View user's profile View All Posts By User
ItalianChemist
Hazard to Others
***




Posts: 180
Registered: 26-1-2011
Location: Italy
Member Is Offline

Mood: No Mood

[*] posted on 11-12-2023 at 04:34


It seems to contain some Iron. Maybe this is the reason why it isn't fluorescent
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1251
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 11-12-2023 at 05:27


Quote: Originally posted by ItalianChemist  

With NaOH only the hydrated hydroxide seems to precipitate.

[Edited on 11-12-2023 by ItalianChemist]


You must add persulfate and heat it in the order to oxidize Tb(OH)3 to Tb4O7.
View user's profile View All Posts By User
ItalianChemist
Hazard to Others
***




Posts: 180
Registered: 26-1-2011
Location: Italy
Member Is Offline

Mood: No Mood

[*] posted on 11-12-2023 at 05:37


Quote: Originally posted by Bedlasky  
Quote: Originally posted by ItalianChemist  

With NaOH only the hydrated hydroxide seems to precipitate.

[Edited on 11-12-2023 by ItalianChemist]


You must add persulfate and heat it in the order to oxidize Tb(OH)3 to Tb4O7.

I have some old persulfate, I will try if it works!
I've seen that it could be obtained also heating the hydroxide to high temperature!
Thank you!
View user's profile View All Posts By User
ItalianChemist
Hazard to Others
***




Posts: 180
Registered: 26-1-2011
Location: Italy
Member Is Offline

Mood: No Mood

[*] posted on 13-12-2023 at 06:11


Ok so I think I can confirm this is Terbium
I got a small sample of the hydroxide and heated until it became red hot for a couple of minutes.
I obtained a black powder that should be Tb4O7, or a mixture of oxides.
The oxide obtained is pretty inert and doesn't seem to react with HCl.
None of the oxide shows any fluorescence



IMG_3053 copia.JPG - 832kBIMG_3054.JPG - 2.4MB
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1251
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 13-12-2023 at 17:22


You can try dissolve Tb(OH)3 in sulfuric acid and make some terbium sulfate. Lanthanide sulfates have very low solubility in boiling water, so you can precipitate most of terbium sulfate by heating the solution. In this way you should obtain pure terbium sulfate, iron contamination stay in the solution (just make sure you have small excess of H2SO4 in the solution to prevent precipitation of iron as basic sulfate).
View user's profile View All Posts By User
ItalianChemist
Hazard to Others
***




Posts: 180
Registered: 26-1-2011
Location: Italy
Member Is Offline

Mood: No Mood

[*] posted on 15-12-2023 at 02:32


Quote: Originally posted by Bedlasky  
You can try dissolve Tb(OH)3 in sulfuric acid and make some terbium sulfate. Lanthanide sulfates have very low solubility in boiling water, so you can precipitate most of terbium sulfate by heating the solution. In this way you should obtain pure terbium sulfate, iron contamination stay in the solution (just make sure you have small excess of H2SO4 in the solution to prevent precipitation of iron as basic sulfate).

Unfortunately all sulfuric acid that I have has a dark color so I think I would end up with a huge mess.
I think I will make Terbium acetate and, for the moment, I will keep that way.
View user's profile View All Posts By User
ItalianChemist
Hazard to Others
***




Posts: 180
Registered: 26-1-2011
Location: Italy
Member Is Offline

Mood: No Mood

[*] posted on 15-12-2023 at 04:39


So it seems that Iron(III) acetate is completely insoluble in water.
Dissolving and acetic acid and filtering should remove the iron. I will try it and post result once I've done.