Polyisobutylene plasticizer extraction
Hi, can I do the plasticizer extraction from these products?
Soudal butyrub
Attachment: TDS_BUTYRUB_2017.pdf (223kB) This file has been downloaded 505 times
Attachment: TDS - Soudal Butyrub Mastic.pdf (125kB) This file has been downloaded 454 times
|
|
underground
National Hazard
Posts: 703
Registered: 10-10-2013
Location: Europe
Member Is Offline
|
|
You could tried it out. Use some benzene and try to extract whatever you can extract. Evaporate and check what you got. But if you want something with
100% results, here is what you have to get.
|
|
kazdo
Harmless
Posts: 2
Registered: 24-6-2019
Member Is Offline
|
|
Ok, thanks a lot . I still have a question, did anyone try to buy pure
polyisobutylene? e.g. from china alibaba?
|
|
underground
National Hazard
Posts: 703
Registered: 10-10-2013
Location: Europe
Member Is Offline
|
|
Those tapes i mentioned will feet your needs 100%. The pib they got may be even better than pure pib for your purpose.
Here is a very good video from LL
https://www.youtube.com/watch?v=euVUa7C5rAM
[Edited on 25-6-2019 by underground]
|
|
Laboratory of Liptakov
International Hazard
Posts: 1405
Registered: 2-9-2014
Location: Technion Haifa
Member Is Offline
Mood: old jew
|
|
PIB from Scapa 2501 (+ 5W40) has better properties than plasticizer - binder in C4 at same content. At usual amateur temperatures of use......LL
Development of primarily - secondary substances CHP (2015) Lithex (2022) Brightelite (2023) Nitrocelite and KC primer (2024)
|
|
Fantasma4500
International Hazard
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
i just wanted to bud in with something i have finally found the name of: TRANSFER TAPE
its essentially adhesive on a roll, but its not adhering to anything else but some type of waxed paper
of what i can find its seemingly some type of acrylic adhesive, it can be had on ebay and per weight of the roll its mostly just adhesive weight
ontop of that i would like to add castor oil is probably best bet to use along with PIB or whatever adhesive since its very thick
https://gyazo.com/513b594f8cb5ff9ae0c3bb19c7d7cc2e
|
|
Raid
Hazard to Everyone
Posts: 203
Registered: 14-11-2022
Location: N/A
Member Is Offline
|
|
I have found that gasoline of just plane hexanes/heptane works well for extracting this.
|
|
dettoo456
Hazard to Others
Posts: 249
Registered: 12-9-2021
Member Is Offline
|
|
I know this’d probably be better categorized in reagents acquisition, but since this topic is already dedicated to it, I’ll just add on.
I recently got my hands on some Oppanol N150 PIB (I believe it’s their highest MW currently produced) and I wouldn’t ever be able to use all of it
on my own so if anyone wants some, I’d happily ship 500g-1kg samples (or less depending on what you want) per person to anyone in the US. I got the
stuff for free so all I’d ask is for the $ to cover shipping.
If anyone in the EU wants in, I can try to figure out shipping but it’d be a little harder to manage.
There’s 10kg in total up for grabs.
|
|
fx-991ex
Hazard to Others
Posts: 100
Registered: 20-5-2023
Member Is Offline
|
|
I got myself some self fusing silicon tape, do you think its the same thing?
Didn't try to extract it yet.
|
|
dettoo456
Hazard to Others
Posts: 249
Registered: 12-9-2021
Member Is Offline
|
|
I don’t think so - definitely contains silicone/ silicone rubbers but I don’t know what the active agent for self-fusing would be. Rat glue is the
most common source for low MW PIB that i know of.
|
|
EF2000
Hazard to Others
Posts: 153
Registered: 10-5-2023
Location: The Steppes
Member Is Offline
Mood: Taste testing the Tonka fuel
|
|
If you can just dissolve it, you can use it without extracting anything. Silicone is a great binder. As seen in that table from article in CEJEM, it decreases sensitivity much more than polymethyl-methacrylate (PMMA usually, but "PA" in table).
I guess PIB is more on PMMA side, so why trying to replicate C-4 when you can make XTX 8004
[Edited on 10-10-2023 by EF2000]
|
|
Microtek
National Hazard
Posts: 872
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
Silicone rubbers are nice for general pbx use, but xtx8004 doesn't remain moldable. Rather, it cures in a matter of days to a rubber. So, if you are
specifically interested in moldable plastiques, you need something that doesn't cure. Reading the LASL entry, I'm struck by this passage:
Quote: |
Charge radius affects the detonation velocity of 1.5-g/cm 3 XTX 8004 confined in polycarbonate plastic in a hemispherical configuration as follows.
|
I wonder how that test works. How do you even initiate a 1.5 mm diameter hemispherical (not cylindrical) charge without the detonator drowning out the
effect of the charge? Also, even if you can do that, there is the question of stable propagation over longer distances.
|
|
EF2000
Hazard to Others
Posts: 153
Registered: 10-5-2023
Location: The Steppes
Member Is Offline
Mood: Taste testing the Tonka fuel
|
|
Quote: Originally posted by Microtek | Silicone rubbers are nice for general pbx use, but xtx8004 doesn't remain moldable. Rather, it cures in a matter of days to a rubber. So, if you are
specifically interested in moldable plastiques, you need something that doesn't cure. |
Sure, but it can be made more moldable by adding silicon oil, can't it?
Quote: Originally posted by Microtek |
I wonder how that test works. How do you even initiate a 1.5 mm diameter hemispherical (not cylindrical) charge without the detonator drowning out the
effect of the charge? Also, even if you can do that, there is the question of stable propagation over longer distances. |
It's even stranger with XTX 8003 (page 192). They somehow tested it down to 0.36 mm.
Alrigth, they explain the method in the second part of book, here. Basically they detonate a long "rate stick" from one end and register wave progress using probes (just like in your apparatus) or smear
camera.
There's more details in the report ACR-221. The piece by Campbell and Engelke cited by LASL is on page 642.
|
|
Microtek
National Hazard
Posts: 872
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
It may be possible to retain the viscous nature of the composite by including a lot of oil to act as the plasticizer, but only experiment will tell if
you also retain the coherency of the plastique. I have done some experiments with silicone based binder/plasticizer composites, and a lot of my
formulations have been fine with regards to mechanical properties, but have suffered from poor shelf life, turning stiff and rubbery over the course
of a few months.
|
|