Author: Subject: 13X molecular sieve
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 6-5-2023 at 16:15
13X molecular sieve


It appears to remove co2 and dries gases.

https://link.springer.com/article/10.1007/s43979-022-00017-5

And it has an appearance change when it needs to be regenerated.

This would be simpler for my book.




Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 13-5-2023 at 19:59


Quote: Originally posted by ErgoloidMesylate  
It appears to remove co2 and dries gases.

https://link.springer.com/article/10.1007/s43979-022-00017-5

And it has an appearance change when it needs to be regenerated.

This would be simpler for my book.


From the paper:

"The molecular sieve is heated to 120 °C to completely remove the adsorbed H2O and CO2"

Not factoring in energy costs, 150C removes slightly more, based on the references.




Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 13-5-2023 at 20:32


I notice that have adjustable regulators between 1 and 10 ATM for compressed air fairly cheap.



Cannula transfer and cannula filtering is used for lysergic synth Compressed air and remove co2
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3721
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 14-5-2023 at 04:30
13x... More than one type


13x aluminosilicate zeolite is probably what you are discussing,
I'm looking for 13x lithium zeolite for oxygen concentrator
Anyone know of a source?

10 bar is the normal pressure for compressed air in uk industry,
hence the 1 to 10 bar regulators are common, cheap and reliable.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
ErgoloidMesylate
Banned
**




Posts: 89
Registered: 8-8-2022
Location: Norad
Member Is Offline

Mood: Freedom of thought is priceless - You can't afford it

[*] posted on 14-5-2023 at 11:59


Quote: Originally posted by Sulaiman  
13x aluminosilicate zeolite is probably what you are discussing,
I'm looking for 13x lithium zeolite for oxygen concentrator
Anyone know of a source?

10 bar is the normal pressure for compressed air in uk industry,
hence the 1 to 10 bar regulators are common, cheap and reliable.


The sieve that adsorbs co2 is widely available by the POUND.

https://www.amazon.com/HFS-Molecular-Sieve-Zeolite-8X12/dp/B...

You want a lithium one, a search states china has them.