Anyone know what I can do with Manganese(III) Oxide
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6269
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
From what source? How pure?
If it is from battery paste then it is a mixture of Mn(III) and Mn(IV) oxides depending on the state of charge. It will also have water and either
ZnCl2 or NH4Cl and impurities.
A lot of Mn compounds have a considerable amount of iron as an impurity.
Nevertheless, it can still be a good start point for Mn compounds. MnCl2 or MnSO4 are usually the next stop. Nurdrage's videos on this process are
good. His ultimate goal was MnO2 plated electrodes.
In a completely different direction, Mn oxides make for a fun thermite.
|
|
Texium
|
Thread Moved 13-3-2023 at 08:57 |
supertater42
Harmless
Posts: 4
Registered: 29-1-2023
Member Is Offline
|
|
i tried researching about the chemistry of manganese(III) oxide because i likely dug some out from a battery, but i didn't find much about it like
what would it react to for example and maybe finding a way to possibly reducing it to manganese dioxide
i'm also a bit new here.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6269
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Purifying battery paste is a good exercise in its own right and one in which you will learn a lot of skills. Nurdrage shows a few methods. I do not
know if anyone has made more recent videos, but the procedures will be similar. Fo not be tempted to substitute HCl for H2SO4. You will gas yourself
with chlorine.
Don't worry about isolating Mn2O3. Instead convert to a Mn(ii) salt. MnO2 will convert at the same time. You cannot separate the graphite from the
oxides without first converting the oxide to something soluble. So not worth trying.
In case you really want the oxide... For most practical uses of tMn(ii) salts they will be oxidised to MnO2 and so you can recover and recycle if you
desire.
Be prepared for it to become messy. And difficult to filter.
|
|
supertater42
Harmless
Posts: 4
Registered: 29-1-2023
Member Is Offline
|
|
sorry if i sounds a bit dumb but can Mn2O3 react to acids?
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4301
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
You should be able to reduce it to Mn(II) with acid (hydrochloric or nitric) and hydrogen peroxide), unless it's calcined.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6269
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
I would be cautious about using nitric or hydrochloric acids -- you will get NO2 or Cl2 gas evolution. No peroxide needed.
I speak from experience here. In my early days as a hobby chemist I managed to fill my shed with chlorine doing exactly this. And it frothed up and
overflowed the beaker as well. I had to evacuate in a hurry holding my breath. Breathing Cl2 is not a whole lot of fun.
Edit
Sulfuric acid works fine. The method with oxalic acid is clever and also works well. Follow Nurdrage.
Don't assume that it is MnO3 that you have. It will be a mixture of oxides. And there will be a lot of graphite powder there as well.
[Edited on 20-3-2023 by j_sum1]
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4301
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Quote: Originally posted by j_sum1 ![](images/xpblue/lastpost.gif) | I would be cautious about using nitric or hydrochloric acids -- you will get NO2 or Cl2 gas evolution. No peroxide needed. |
The peroxide is a useful reducing agent to make sure you don't get chlorine or NO2.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6269
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Ok. I normally use peroxide as an oxidiser.
If this works, fine.
My inclination with anything new is to test at small scale first.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7997
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Normally, hydrogen peroxide is used as oxidizer, but in this specific case, it is a wonderful reductor. If you have brown stains or a brown mud of
hydrous MnO2 and/or hydrous Mn2O3, and you add dilute acid, to which some hydrogen peroxide is added, then you get instant reduction of the
manganese(III) and/or manganese(IV) to manganese(II). This reaction is very fast and complete. It only works at low pH though. At high pH, peroxide
instantly oxidizes manganese(II) to manganese(IV).
Peroxide also instantly reduces permanganate to manganese(II) at low pH and at (near-)neutral pH, it reduces permanganate to manganese(IV). The
manganese(IV) then also acts as a powerful catalyst for decomposition of H2O2.
|
|
Fantasma4500
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline
Mood: dangerously practical
|
|
NaOH and a sugar should cause it to turn into MnO or similar lower oxide which shouldnt oxidize acids, then it should be able to react with HCl to
make MnCl2
otherwise oxidize it into MnO2 and melt with NaOH for some interesting color chemistry, permanganate
|
|