Does anyone here know of a way to fully dissolve carbon (graphite form) ?
I am not talking about removing graphite burn stain or finely divided powder suspension in a liquid. I mean fully dissolving it like table salt in water ? or rather sugar ... I thought about carbon disulfide possibly ? anything else?
The goal is to bypass the tedious, long and error prone process for preparing sample for carbon dating . Which by the way must mix with a toluene based scintillation solvent... any idea?


https://www.youtube.com/watch?v=qvi83-PTDN8

C14 dark.jpg - 473kB
View user's profile Visit user's homepage View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4360
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 5-1-2022 at 17:15


I don't think carbon dissolves in much other than molten iron. Definitely not toluene or carbon disulphide.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4622
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: PhD candidate!

[*] posted on 5-1-2022 at 18:09


Piranha solution or chromic acid are all that come to mind for me, though those would likely damage your sample.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1244
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 5-1-2022 at 19:39


Quote: Originally posted by Texium  
Piranha solution or chromic acid are all that come to mind for me, though those would likely damage your sample.


Concentrated nitric acid should also work (in theory). But I never tried that. Fenton should also oxidize it to CO2.




View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 5-1-2022 at 21:02


Chlorosulphonic acid is the only solvent other than iron.

https://www.nature.com/articles/nnano.2010.86
View user's profile View All Posts By User
MichaelBijanAfghani
Harmless
*




Posts: 19
Registered: 15-11-2021
Member Is Offline


[*] posted on 5-1-2022 at 21:10


Quote: Originally posted by Texium  
Piranha solution or chromic acid are all that come to mind for me, though those would likely damage your sample.

Maybe You could bubble the outgoing carbon dioxide into water to make carbonic acid, then add sodium hydroxide to get sodium carbonate.




View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1244
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 5-1-2022 at 21:24


Quote: Originally posted by MichaelBijanAfghani  
Quote: Originally posted by Texium  
Piranha solution or chromic acid are all that come to mind for me, though those would likely damage your sample.

Maybe You could bubble the outgoing carbon dioxide into water to make carbonic acid, then add sodium hydroxide to get sodium carbonate.


It would be better CO2 directly to NaOH solution. If you bubble CO2 just to the water, some will escape to the air.




View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 6-1-2022 at 01:49


Do you know what form the 14C is in?
I seem to recall that it is made by irradiating nitrogen with neutrons or something.
If I was doing that, I'd use a nitrate salt to hold the nitrogen in place in the reactor and then precipitate the carbonate that's formed with calcium or some such. (You would need a carrier).
In that case, the answer to your question might be that you can dissolve it in vinegar.
View user's profile View All Posts By User
neptunium
National Hazard
****




Posts: 990
Registered: 12-12-2011
Location: between Uranium and Plutonium
Member Is Offline


[*] posted on 6-1-2022 at 03:59


I realize now that the picture is a bit misleading... the carbon in the source is on a waxy substance i had no trouble dissolving in toluene for my reference 14C.
I am currently measuring unknown samples (video) by first heating in absence of oxygen to make it a chunk of charcoal. this is then burned in oxygen and the CO2 produced bubbles in a concentrated solution of LiOH which rapidly precipitate as lithium carbonate. this Li2CO3 can be somewhat dissolved in my scintillation cocktail for counting but this is not an ideal process.
A better way would be to add dropwise a dilute solution of HCl in a vacuum to recover the clean CO2, react it with Lithium metal to get the carbide which releases acetylene when dropped in water. this C2H2 can be heated in a steel catalyst to cycle into benzene .
That carbon rich benzene is then weighted and dissolved in the scintillation cocktail for counting .
So clearly the sample is completely destroyed in the process which is fine . But this is a high waste generating process with many opportunity for contamination and I wanted to come up with a better/easier way to prepare samples from graphite to a carbon liquid easily dissolved in the scintillation cocktail (mostly made of toluene BTW).
The best way I came up with was to react the charcoal directly with sulfur at high temp and distill away the CS2 .
Molten Iron is out of the question for obvious reason
I do not believe HNO3 would do much at all but it`s worth trying
I also heard about hot concentrated sulfuric acid and this is also worth trying (although probably also very inefficient)
Chlorosulphonic acid is the one that keeps coming back in many articles, I`d like to try it out but obtaining it may be a challenge ...
Thank you all or your contribution I do appreciate it ! :)
View user's profile Visit user's homepage View All Posts By User
WGTR
National Hazard
****




Posts: 971
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 6-1-2022 at 06:43


The conversion of CO/CO2 and H2 to methanol is performed catalytically on a large scale, if you're trying to perform a gas-to-liquid hydrocarbon-type reaction. It would probably be difficult to do on a lab scale and not very efficient though. Good luck.



View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 6-1-2022 at 14:36


chlorosulphonic acid requires either fuming oleum or phosphorus pentachloride to make.

Assuming you are starting with an organic mixture, a better method may be to use caro's acid aka piranha solution.
This will convert the carbon directly to CO2 without the carbonization step.
Then capture in lithium carbonate solution.

This eliminates one step.
The fewer steps the less room for loss or contamination.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 6-1-2022 at 14:49


I think the yield of the acetylene to benzene reaction is poor, with lots of by products.
On the other hand, acetylene is probably reasonably soluble in toluene.
How about reaction of CO2 with a Grignard , for example phenylmagnesium bromide to make benzoic acid?

The old school approach was to mix the sample with excess copper oxide and then heat it to convert all the carbon present to CO2.
No need for an intermediate charcoal step (with possible losses).

I think the apparatus was a flow of nitrogen through a a hard glass tube with copper oxide to oxidise the organics to CO2 H2O etc, then copper turnings to reduce any NOx to N2 Then silver to remove halogens and finally phosphoric acid to remove most of the water.
After that you have pretty clean CO2 in N2

View user's profile View All Posts By User
neptunium
National Hazard
****




Posts: 990
Registered: 12-12-2011
Location: between Uranium and Plutonium
Member Is Offline


[*] posted on 7-1-2022 at 03:39


Quote: Originally posted by macckone  


Assuming you are starting with an organic mixture, a better method may be to use caro's acid aka piranha solution.
This will convert the carbon directly to CO2 without the carbonization step.
Then capture in lithium carbonate solution.

This eliminates one step.
The fewer steps the less room for loss or contamination.


I like that... the loss aren`t important . a few milligram suffice and there is usually plenty of sample available . Contamination on the other hand IS a big issue and eliminating a step is a huge benefit!




[Edited on 7-1-2022 by neptunium]
View user's profile Visit user's homepage View All Posts By User
neptunium
National Hazard
****




Posts: 990
Registered: 12-12-2011
Location: between Uranium and Plutonium
Member Is Offline


[*] posted on 7-1-2022 at 03:47


Quote: Originally posted by unionised  
I think the yield of the acetylene to benzene reaction is poor, with lots of by products.
On the other hand, acetylene is probably reasonably soluble in toluene.
How about reaction of CO2 with a Grignard , for example phenylmagnesium bromide to make benzoic acid?

The old school approach was to mix the sample with excess copper oxide and then heat it to convert all the carbon present to CO2.
No need for an intermediate charcoal step (with possible losses).

I think the apparatus was a flow of nitrogen through a a hard glass tube with copper oxide to oxidise the organics to CO2 H2O etc, then copper turnings to reduce any NOx to N2 Then silver to remove halogens and finally phosphoric acid to remove most of the water.
After that you have pretty clean CO2 in N2



That sounds good but the introduction of Phenylmagnesium is the source of contamination since it already contain carbon . Even as a petroleum byproduct there is no way to get reliable result not knowing the history of the chemical. Nitrogen is a much better option than burning charcoal in O2 I agree !