Sn + HNO3 => Sn(NO3)2 - tin(II) nitrate
Hello,
What happens when you put some tin in nitric acid?
Maybe with a conc of between 1 to 10 M.
Does [[Sn3(OH)4]2](+) [NO3](-) form in water? Does it decompose forming SnO?
Wikipedia does not document tin(II) nitrate.
There is only tin(IV) nitrate.
Another site, a forum, mentions that dry tin(II) nitrate can’t be prepared but you can have Sn(NO3)2.20 H2O
There is this page
https://www.sciencedirect.com/science/article/abs/pii/002016...
but that is a single page preview.
Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
|
|
Bedlasky
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline
Mood: Volatile
|
|
Tin reacts with nitric acid to produce hydrous SnO2. You cannot produce any tin nitrate in aqueous solution.
I once analysed some Sn-Pb-Cu alloy. I dissolved it in nitric acid, filter off SnO2.xH2O and by strong heating converted it to anhydrous SnO2. Pb was
determined as PbSO4 and Cu by iodometry.
|
|
vmelkon
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline
Mood: autoerotic asphyxiation
|
|
Actually, I am trying to separate some Sn-Cu-Ag alloy.
HCl dissolves the Sn. What is left is a red powder that slowly produces bubbles, so I assume it still contains some tin.
My plan was to use HNO3 to dissolve this powder but looks like some insoluble yellow white substance formed, so I think this is the SnO2.
Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
|
|
S.C. Wack
bibliomaster
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline
Mood: Enhanced
|
|
With cooling and an excess of acid diluted with at least 3/4 volume of water, tin is said to give a colorless solution of stannous nitrate...and
ammonium nitrate, which are not particularly separable or isolated as such. Hydrolysis products would depend on all of the variables...it is said that
the yellow-white substance is a mixture of white stannic nitrate and a yellow basic stannic nitrate.
|
|