[*] posted on 8-11-2021 at 02:10
Reducing organic compounds with devarda's alloy?


I have a large jar of powdered Devarda's alloy that was once used for the analysis of nitrite and nitrate salts. Recently I was wondering if it could be used to replace other aluminium alloys as a reducing agent for organic compounds such as nitro compounds in alkaline solution.

Has anyone ever tried it as an organic reducing agent? It has been discussed before on SM as a possible reducing agent for PETN but I thick the alkaline solution required would cleave the nitrate groups in this case. I would imagine that it functionality would be similar to Al-Ga and Al-amalgam.
View user's profile View All Posts By User
Fery
International Hazard
*****




Posts: 1029
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline


[*] posted on 8-11-2021 at 02:45


Hi Boffis, I did not try, but have this - reduction of nitrobenzene to hydrazobenzene using Dewarda's alloy.

Attachment: vogel1958.pdf (927kB)
This file has been downloaded 291 times




View user's profile Visit user's homepage View All Posts By User
Boffis
International Hazard
*****




Posts: 1886
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 8-11-2021 at 05:46


Hi Fery, many thanks for that paper! I think I can feel some experimental chemistry coming on! Devarda's alloy crops up on ebay fairly frequently in the UK and its cheap.
View user's profile View All Posts By User
arkoma
Redneck Overlord
*******




Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline

Mood: украї́нська

[*] posted on 8-11-2021 at 21:12


Interesting. I've got a furnace that gets hot enough to melt copper.




"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
SWIM
National Hazard
****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 9-11-2021 at 00:09


Might not even need to reach copper's melting point.

Molten aluminum will dissolve copper to some extent.

I just checked and the alloy boils at 906 C, so hopefully it can be made below that temperature.





View user's profile View All Posts By User
arkoma
Redneck Overlord
*******




Posts: 1763
Registered: 3-2-2014
Location: On a Big Blue Marble hurtling through space
Member Is Offline

Mood: украї́нська

[*] posted on 9-11-2021 at 10:52


melted 25gm Cu, 22.5gm Al and 2.5gm Zn. Now just to figure out a use for it........



devardas.jpg - 2.5MB




"We believe the knowledge and cultural heritage of mankind should be accessible to all people around the world, regardless of their wealth, social status, nationality, citizenship, etc" z-lib

View user's profile View All Posts By User
Fery
International Hazard
*****




Posts: 1029
Registered: 27-8-2019
Location: Czechoslovakia
Member Is Offline


[*] posted on 9-11-2021 at 11:45


arkoma - well done and beautiful! Is the alloy fragile so could be grounded to dust? All my Dewarda's alloys are are very fine particle dust. Or is it so reactive that it does not require pulverization?



View user's profile Visit user's homepage View All Posts By User
SWIM
National Hazard
****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 9-11-2021 at 16:10


So is this stuff basically an activated form of aluminum?

Like aluminum/mercury amalgam?

Be nice to find a less toxic substitute for that.

edit: I have heard of copper activated zinc being used for some of the same reactions as Al/Hg.



[Edited on 10-11-2021 by SWIM]




View user's profile View All Posts By User
Triflic Acid
Hazard to Others
***




Posts: 486
Registered: 27-9-2020
Member Is Offline

Mood: Slowly Oxidizing into Oblivion

[*] posted on 9-11-2021 at 17:05


Would be interesting if this could be used for a Clemmensen reduction, since it has a decent zinc quantity



There wasn't a fire, we just had an uncontrolled rapid oxidation event at the power plant.
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1886
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 9-11-2021 at 20:09


@ Swim, yes I think you are right that's why I was asking about its similarity with aluminium amalgam etc. Given the amount of discussion on this forum given over to the aluminium-gallium alloy and related mixtures I thought this stuff seem to be a more accessible and cheaper alternative still. Also its mercury free!
View user's profile View All Posts By User

  Go To Top