Author: Subject: Decomposition of hydrogen peroxide on the surface of copper
vano
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 9-11-2021 at 05:39
Decomposition of hydrogen peroxide on the surface of copper


Hi. I have a new experiment. I think you will be interested. I made solution of peroxotungstic acid. i added tungstic acid in 50% peroxide solution, next when i added copper oxygen began to be released intensively, like MnO2+H2O2 reaction. i also tryed zinc, but because its active metal its very dirty reaction, black particles was everywherein solution. also silver and other metals, but copper is fastest and also inert (silver produced insoluble tungstarte very easily), end of the reaction solution had greenish colour. interesting how its works on for example platinum. as i know formula of this peroxocompound is H2[WO(O2)2(OH)2]

251586558_1047236696066349_1905571097533971037_n.jpg - 523kB 250872491_293130226017409_2927126041641062815_n.jpg - 504kB

250717143_1089297674940272_5278267115900090812_n.jpg - 178kB 11.jpg - 214kB

[Edited on 9-11-2021 by vano]

[Edited on 9-11-2021 by vano]

[Edited on 9-11-2021 by vano]

[Edited on 9-11-2021 by vano]




View user's profile View All Posts By User
Fantasma4500
International Hazard
*****




Posts: 1681
Registered: 12-12-2012
Location: Dysrope (aka europe)
Member Is Offline

Mood: dangerously practical

[*] posted on 9-11-2021 at 08:04


interesting, maybe you will have a catalyst named after you soon? try to avoid becoming easily assasinated for now. you should try and see if this can react with other oxygen like compounds, chlorates maybe



~25 drops = 1mL @dH2O viscocity - STP
Truth is ever growing - but without context theres barely any such.

https://en.wikipedia.org/wiki/Solubility_table
http://www.trimen.pl/witek/calculators/stezenia.html
View user's profile View All Posts By User
vano
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 10-11-2021 at 00:11


as i know this peroxocomplex is stable only in solution and if we want to make oxygen from KClO3 we need catalysis, for example MnO2 and heat. i dont think something will happen in solution. Maybe you meant something else and I could not understand you, tell me in more detail.