pembinariver
Harmless
Posts: 1
Registered: 12-6-2018
Member Is Offline
|
|
How to make potassium sulfide from potassium sulfate?
According to Wikipedia:
Quote: | [Potassium sulfide] can be produced by heating K2SO4 with carbon (coke):
K2SO4 + 4 C → K2S + 4 CO |
Unfortunately there are no references for this, so I don't know where to look for more information.
Someone on chemicalforums.com told me the reaction should happen around 915K. Wikipedia says K2S would decompose at 1185K so I'll have to keep the
reaction below this.
I was thinking of heating potassium sulfate with milled charcoal in the absence of oxygen. Is there anything I'm missing here?
|
|
Triflic Acid
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 486
Registered: 27-9-2020
Member Is Offline
Mood: Slowly Oxidizing into Oblivion
|
|
Welcome to SM. You might have some trouble storing the K2S, it is extremely hydroscopic. What do you need it for that you can't use something nicer
like sodium sulfide?
There wasn't a fire, we just had an uncontrolled rapid oxidation event at the power plant.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
There's a fair bit of data on the comparable reduction of BaSO4.
That might give you some hints.
One of the more important considerations is that hot sulphides will oxidise in air; you need to exclude that until the material cools.
|
|