Pages:
1
2 |
Mateo_swe
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 528
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
Storage of 35% H2O2
I recently bought 2L of 35% H2O2.
I currently have them in roomtemp and the plastic PE bottles are getting pressurized by the H2O2 so i have to release the pressure every day.
Do i need to store the bottles in a refridgerator for the H2O2 to stop develop pressure?
I know H2O2 can build up pressure when stored but releasing pressure every day seem way to often.
It say on the label the 35% H2O2 is stabilized.
Can it be that the bottles are not in complete darkness? and how much pressure should 35% H2O2 build up over time during storage?
I have had 35% H2O2 many years ago and that bottle didnt have this problem with built up pressure in the bottle, at least not in this amount that i
have in these new bottles.
Any ideas?
|
|
teodor
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 875
Registered: 28-6-2019
Location: Heerenveen
Member Is Offline
|
|
Indeed, I have no problems with storing 25% H2O2 at room temperature in normal light conditions but my bottle with 10% H2O2 is building pressure every
day after some day when I put some liquid back to the bottle from a beaker. I suspect that trace amount of transitional metals/oxides/salts is the
main reason for this effect, not H2O2 concentration/light/temperature.
[Edited on 22-7-2021 by teodor]
[Edited on 22-7-2021 by teodor]
|
|
Bedlasky
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline
Mood: Volatile
|
|
Oxygen pressure is good thing, it prevents decomposition. I store H2O2 in brown glass bottle without issues.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3649
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
The vapour pressure of hydrogen peroxide is quite low,
so low that a sealed container does not need venting.
As above, I keep my 50% solution pressurised
Maybe something in the container is catalysing decomposition?
Try re-bottling in a clean container?
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Mateo_swe
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 528
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
Hmm, the PE plastic bottles were brand new, unused and i washed them with water before i put the H2O2 in them.
So i can use a glass bottle to store the H2O2 and the built up pressure would not break the bottle or screw on cork?
The H2O2 was in different plastic bottles when purchased, but on arrival one bottle was looking like a ballon and the other had got a leak in the
screw on cork from the pressure buildup.
Can a rough, bumpy shipping by truck make the H2O2 build up pressure like this?
I changed the bottles but the pressure buildup continues, i dont knoiw if i dare put the H2O2 in glass bottles.
It would be best to have it in glass reagent bottles but maybe they crack from the pressure.
|
|
karlos³
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline
Mood: oxazolidinic 8)
|
|
Is the stuff stabilised?
I measured the density of some 30% H2O2 I bought like... uh... six or seven years ago or so, and according to the density it was(stabilised) still a
good bit over 20%.
I think it keeps pretty well in that case.
|
|
Fyndium
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1192
Registered: 12-7-2020
Location: Not in USA
Member Is Offline
|
|
Washed with.. tap or distilled/deionised water? It can make a huge difference. If I've read right, some metals like platinum can cause explosive
decomposition, and lesser metals can likely do so at a more protracted rate. Yet still, storing it in a closed bottle, even with little decomposition
would build up pressure until the bottle simply bursts. Since some sturdy bottles can withstand up to 10bar of pressure before going off, it can be
quite the blast.
Now that I remember, my canister of H2O2 has got a pressure compensated cap, hence it doesn't seemingly build pressure. It was stored in cold over
winter, and during hottest summer days the temp raised above 20C and some bubbles were lodged to the interiors of the can.
|
|
Panache
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
Storage for such items can be fraught. Repackaging can often worsen the problem. If you are considering repackaging glass cleaned with hot dilute
nitric acid plus several hot rinses with validated pure water is your best bet. Afterward cap and store bottle in a mild steel tube. Open only with a
socket wrench such that line of sight to closure is impaired. This would be the only safe method (yet still fraught) as you dont know what is causing
your decomposition.
|
|
Mateo_swe
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 528
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
It says on the label:
Deka Fine Chemicals
Hydrogen Peroxide 35%, Pure, Stabilized.
It also says:
Store in room temperature 2-25°C, store in a dry, well ventilated environment, store with bottle tightly closed, store locked up.
Stable under recommended storage conditions.
So it should be stable and not build up pressure like this.
When i changed bottles i used brand new PE plastic bottles rinsed with tap water, there was no water left in bottles but might have been some very
small amount.
Since the H2O2 was building up pressure even in the bottles it was shipped in, the problem seem to have been present from the start.
I have no steel cylinders to store glass reagent bottles in.
Can one buy these pressure compensated caps you have on your bottle Fyndium?
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I am afraid that something is wrong with your H2O2 and that it has slight contamination with some catalyst. Even trace amounts, which have no effect
at all in other reactions, can still lead to decomposition at a fairly high rate. In the past I had 30% H2O2 and this indeed did decompose, but very
slowly. I had pressure buildup in weeks or months. After a few days of storage, I did not have any noticeable pressure builduip. Right now, I still
have 10% H2O2 and this also is quite stable on storage. I have that bottle for more than two years now and it still is nearly as potent as when I
purchased it.
For now, I certainly would NOT store the H2O2 in tightly sealed bottles. Keep the bottles loosely capped and assure that they remain upright in your
storage cabinet. The oxygen outgassing is no problem for other nearby bottles and if you have the caps loosely sealed, you will have no noticeable
vapors of water or H2O2.
I expect that your H2O2 will have lost its oxidizing properties within months if you have such severe pressure issues. I would convert the H2O2 to
something more stable. E.g. with sodium borate or borax you can make sodium perborate, which is easily separated and has infinite shelf life. Or use
it up in syntheses before it has decomposed.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Bollocks.
At any pressure that you could plausibly contain, the effect will be tiny.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Mateo_swe ![](images/xpblue/lastpost.gif) | H
So i can use a glass bottle to store the H2O2 and the built up pressure would not break the bottle or screw on cork?
|
It certainly will break the stopper or, the bottle if you allow it to build up..
|
|
S.C. Wack
bibliomaster
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline
Mood: Enhanced
|
|
3% peroxide may be found in dark plastic flip-top bottles. These are convenient containers for the same peroxide which has been concentrated to 35%;
this concentrate is not to be expected to be perfectly stable nor is the cap expected to immediately release all pressure. As this can release some
120 volumes of oxygen, a concentrated peroxide which has developed much pressure which has been released many times over the years has actually lost
little of its potency.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3649
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
I bought 1l of 50% hydrogen peroxide 15 months ago and transfered it to a 1l korken (Ikea) bottle.
It has been used a few times, and stored in a cupboard outdoors (25-30C night, 35-40C day).
So I just checked it's concentration by density: 47%
Unfortunately I did not test the concentration on arrival so no reference.
There may have been some significant decomposition, and the bottle may have vented (or leaked).
So
I would like to correct my post above to add:
your storage vesel should have some kind of pressure relief mechanism.
................................................................
P.S. When I was measuring the density I noticed a very small stream of tiny bubbles in the volumetric flask,
even though I had washed the flask with detergent, rinsed, dried, KOH, rinsed, HCl, rinsed, and finally a rinse with some of the H2O2.
Clearly H2O2 does not need much to decompose it.
[Edited on 25-7-2021 by Sulaiman]
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
Chem Science
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 122
Registered: 30-7-2018
Location: Argentina
Member Is Offline
|
|
I store my 70% peroxide between -10º and -15ºC, And at some time i decap the bottle to release the pressure, which is very little.
And the pressure is really low, i hear a slightly degassing noise only.
I agree with Sulaiman on the pressure relief mechanism, it's a very nice safeguard, especially in the case of there been other chemicals in the same
space.
|
|
Mateo_swe
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 528
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
Quote: Originally posted by woelen ![](images/xpblue/lastpost.gif) | I am afraid that something is wrong with your H2O2.
I expect that your H2O2 will have lost its oxidizing properties within months if you have such severe pressure issues.
I would convert the H2O2 to something more stable. E.g. with sodium borate or borax you can make sodium perborate, which is easily separated and has
infinite shelf life. Or use it up in syntheses before it has decomposed. |
Yes there is certainly something wrong with this H2O2, i still have to release the pressure in both my 2 bottles of 1L 35% H2O2 at least once every
day to prevent the plastic bottles to break.
I expect the strength of the H2O2 to decline quite fast so i must do something.
I do have about a kilo of Borax so the best seem to convert it to some Sodium Perborate as this could be useful and stores well.
I will look up the procedure how its done.
Thanks to everyone for the advice and info on my problem.
|
|
Mateo_swe
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 528
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
I found the SM thread about preparation of sodium perborate and also the Prepchem preparation of sodium perborate.
The prepchem procedure uses 3% H2O2 and apparently it seems to weak for good results, at least it seem so reading the SM thread.
My H2O2 is probably still much better than 3%, i havent measured its density yet.
Do you think this Prepchem procedure will work if i re-calculate the amount of H2O2 needed depending on my current strength of the H2O2?
The Prepchem Sodium Perborate preparation:
Na2B4O7 + 2NaOH + 4H2O2 -> 4NaBO3 + 5H2O
24g of borax and 5g of sodium hydroxide are dissolved in 150 ml of warm water. The solution is cooled to room temperature and add 283 ml of 3%
hydrogen peroxide are added slowly. The solution is cooled additionally with stirring by immersing the beaker in ice water and dropping 20 grams of
ice into the solution. After a few minutes, fine crystals of sodium perborate begin to separate. The solution is stirred frequently for the next 20
minutes, then the crystals are collected by filtration, washed with two successive portions of 25 ml each of ethyl alcohol and then two successive
portions of 25 ml each of ethyl ether. Finally, sodium perborate is dried and preserved in a stoppered bottle. Sodium perborate obtained by described
method contains four molecules of water (sodium perborate tetrahydrate), which at 70° C becomes hygroscopic sodium perborate monohydrate.
Some things i wonder about the above prepchem method, can IPA wash be used instead of ethyl alcohol wash?
IPA is anhydrous, or very close to anhydrous and i have a lot of it compared to ethyl alcohol that i only have in anhydrous form and its expensive.
Also is the second ethyl ether wash needed?
I do have diethyl ether, but i rather skip the ether wash if its not needed.
Prepchem Sodium Perborate preparation:
https://www.prepchem.com/synthesis-of-sodium-perborate/
SM Sodium Perborate thread:
http://www.sciencemadness.org/talk/viewthread.php?tid=71240#...
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I think that with much higher concentration than 3% your preparation works better. With 3% you get dilute solutions and then it is more difficult to
get crystals of sodium perborate.
If you have K2Cr2O7 or K2CrO4 (or CrO3), then you also could try making the interesting compound K3CrO8. I would not make more than 20 grams or so of
that, but it is a really interesting prep. This stuff also stores well if you rinse it well after preparation: https://woelen.homescience.net/science/chem/exps/K3CrO8_synt...
With K3CrO8 you can do many interesting experiments, it has energetic properties.
Another interesting peroxo complex is the following: https://woelen.homescience.net/science/chem/exps/Cr_ammine_p...
This one should only be made in small quantities and always keep in mind that this material may ignite unexpectedly (e.g. because of static
discharge). But as long as your H2O2 is strong, it is a really interesting prep.
I also made calcium peroxide from concentrated H2O2 in the past (from Ca(OH)2 and conc. H2O2). Yield was low though and I found it not really
satisfying. The compound is impure and only somewhat energetic.
If you have vanadium pentoxide or some vanadate, you can make an energetic and interesting peroxovanadate, which also kan be kept around indefinitely:
https://woelen.homescience.net/science/chem/exps/KVO4/index....
I still have the KVO4 from that experiment (it's many years old now) and it still is as good as when I made it.
----------------------------------------------------
Rinsing with IPA works well. It works as well as rinsing with ethanol in my experience. A final rinse with ether is very pleasant, because of the
quick drying. You could also use acetone for a final rinse, but keep in mind that acetone is more reactive and certain chemicals may react with that.
But if IPA or ethanol does not react, then I also expect acetone to be non-reactive, at least with dry crystalline inorganic compounds.
[Edited on 29-7-21 by woelen]
|
|
Bedlasky
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline
Mood: Volatile
|
|
Woelen: Calcium peroxide is the worst metal peroxide for synthesis. It is unstable and goes through filter during filtration. SrO2 and BaO2 are stable
and more easy to prepare. I made SrO2 myself and analyse the product. It had very good purity.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I tried making CaO2, simply because I had Ca(OH)2 and CaO, while I did not have the corresponding Sr- and Ba-compounds. Sometimes you just have to use
what you have, even if not optimal. But I agree with you, making CaO2 is not a very satisfying thing. For that reason I also did not make a webpage
about that experiment.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3649
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
You could pipe the oxygen generated by your bottle of decomposing peroxide to a gas collector and see if it really is decomposing quickly - or maybe
less than you fear.
eg a typical 'gas collection by water displacement' setup.
https://www.google.com/search?q=gas+collection+by+water+disp...
You could then estimate how urgent the problem is.
PS The cost and effort of converting to perborate seems high to me,
'oxy' laundry powder or similar is less expensive (I bought mine as sodium percarbonate)
and I think almost as useful?
[Edited on 29-7-2021 by Sulaiman]
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
teodor
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 875
Registered: 28-6-2019
Location: Heerenveen
Member Is Offline
|
|
I suspect that gas collection by water setup will not work well for low gas flow. O2 will go easily through water driven by the difference of partial
pressure in the H2O2 bottle and in the air.
Once I used decomposing H2O2 to prepare BaO2 hydrate, the procedure is not complex except may be drying.
|
|
Bedlasky
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline
Mood: Volatile
|
|
Woelen: I once did small project to make several metal hydroxides - I made MgO2, CaO2, SrO2 and ZnO2. I mixed soluble metal salt solution, hydrogen
peroxide and NaOH to get peroxide. You don't need to isolate metal hydroxide, you can make it in situ. And CaO2 synthesis was the worst from all. Even
MgO2 synthesis was easier than this (despite the fact that MgO2 is less stable than CaO2). CaO2 and MgO2 were heavily contaminated with hydroxides.
Maybe I revesit this project some time (but just Sr, Ba and Zn peroxides) and try some energetic mixtures with these peroxides. I am also interested
in CuO2, but this experiment is better to do in winter, because of instability of CuO2.
[Edited on 29-7-2021 by Bedlasky]
|
|
teodor
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 875
Registered: 28-6-2019
Location: Heerenveen
Member Is Offline
|
|
Also there is hydrogen peroxide - urea complex which is probably is the accessible way to protect H2O2 from decomposition and use it as H2O2 later.
|
|
karlos³
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline
Mood: oxazolidinic 8)
|
|
Quote: Originally posted by teodor ![](images/xpblue/lastpost.gif) | Also there is hydrogen peroxide - urea complex which is probably is the accessible way to protect H2O2 from decomposition and use it as H2O2 later.
|
I have way too much urea and I worry about decomposition of my H2O2.
What would you suggest teo?
Do you have some references that seemed to you like they are simple and harmless to do, and how to revert to the free peroxide without distillation,
etc?
|
|