High speed chips from chiseling
The usual advice for the care of cold chisels is to grind off the mushroomed head to avoid the dangers of flying metal chips. I have never had a
problem of flying metal chips or I hadn't until yesterday.
I was using a cold chisel to attempt to prise off a sleeve from a shaft On one swift hit of the chisel with a hammer I felt an intense pain in one of
my fingers which began to bleed. Apparently a flying small chip of metal had punctured the end of my middle finger. The chisel was new and not
mushroomed. On consideration of the position of the puncture in relation to the chisel, the chip was probably piece of the hardened (assumed) steel
sleeve.
Unfortunately today the area round the puncture is red and tender. I had assumed the chip was large compared to puncture. I checked with a strong
magnets, I can feel an attraction so the metal chip is under the skin The metal chip must be small but was moving so fast it is now a millimeter or
more below skin surface.
When I have dug the metal chip out I will take a picture of it and post it. When the wound was fresh I may have been able to pull the chip with the
strong magnet. No MRIs for me.
Of course the morel of the story is wear hand and eye protection for such operations.
PS: I manged to get the chip out. Its about 2 x 3 mm across and much less than millimeter in thickness. Probably a few mg in mass. I am very
surprised it had sufficient velocity to penetrate the relatively tough
skin of my finger tip.
[Edited on 6/21/2021 by wg48temp9]
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
zwt2
Harmless
Posts: 17
Registered: 3-9-2019
Member Is Offline
Mood: CHoCoLaTe
|
|
Quote: | the morel of the story |
"Since you belong to the small number of wise men... tell me, how do you occupy yourselves?"
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I'm not sure of the date, but the tree we were dropping was an elm- it had Dutch elm disease. That suggests about 1975 and that's close enough.
I wasn't really doing much- I was a schoolkid. But I was "helping out" in the way kids do.
The tree was down and we (well, the adults) were breaking up the tree so they could burn it.
And they were using wedges and a sledge hammer.
The bit that came off the mushroomed head of the wedge hit my right thumb- just where the nail bed ends.
I was young, so the wound healed quickly enough, but the nail on that thumb is still distorted.
So, yes, it's an important issue which is easy to overlook.
If the heads on the wedges are getting mushroomed, grind them back to shape.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I see you are the Fun Guy around here.
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 774
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
Below is a pic of the steel chip on the mm scale of a ruler. There is a magnet holding the ruler and the chip.
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1477
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
High speed (tool) steel... Well a razor blade. Carefully drug across finger at a low/med speed (to be read as, accidentally gored myself) in an
attempt to cut out a drywall crack prior to mudding. Was on an outside angle of the wall next to a light switch. It's not deep, I'm fairly thick
skinned. But I immediately felt super bright about then.
![IMG_20210623_224239105.jpg - 2.1MB](https://www.sciencemadness.org/whisper/files.php?pid=662089&aid=89139)
Painters tape and triple antibiotic ointment = win.
![IMG_20210623_230745.jpg - 1.2MB](https://www.sciencemadness.org/whisper/files.php?pid=662089&aid=89141)
Note the offending knife, broken face paper section of drywall and blood offering on floor. The moral of the story here, drink more coffee doing
afterhours side work. Or just don't try to catch metal with skin meats. Or, keep first aid essentials on hand... There are a few lessons.
|
|