Author: Subject: Recovery of styrene monomer from polystyrene
Keras
National Hazard
****




Posts: 931
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 28-4-2021 at 04:56
Recovery of styrene monomer from polystyrene


Folks,

I have (or rather: used to have) a one litre bottle of styrene, that I left in store somewhere. When I turned back to it, all the styrene had polymerised, so it’s now a bottle full of white polystyrene.

If I wanted to recover the monomer from its present form, what should I do? I read here that heating polystyrene at 400 °C over a MgO bed can led to around 70% styrene recovery. By chance, any other method you'd know that'd require less heat, maybe ?

Thanks.
View user's profile View All Posts By User
njl
National Hazard
****




Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 28-4-2021 at 05:08


The gist of polystyrene to styrene monomer is mostly thermal cracking as far as I know. There are some catalysts like metal oxides (MgO) that can either increase recovery or lower the reaction temperature, but you will still have to use high heat. UC235 has a video on polystyrene cracking on youtube.



Reflux condenser?? I barely know her!
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 28-4-2021 at 06:07


I'm just guessing but 70% seems rather on the low side. Doesn't the uc235 video
Show a much higher yeild using no catalyst?
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2284
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 28-4-2021 at 07:31


Yields via pyrolysis are pretty good.

For some unknown reason, this video isn't starting at the beginning.

https://www.youtube.com/watch?v=6tEs7P6UUVQ

[Edited on 28-4-2021 by zed]
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 28-4-2021 at 08:24


It used to be a classic school demo.
Just heating the stuff will give you styrene.

But, unless you have some hydroquinone or something to use as a polymerisation inhibitor, it will revert to a polymer again.

Also works with PMMA
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 931
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 28-4-2021 at 10:53


Quote: Originally posted by unionised  
It used to be a classic school demo.
Just heating the stuff will give you styrene.
But, unless you have some hydroquinone or something to use as a polymerisation inhibitor, it will revert to a polymer again.
Also works with PMMA


Oh, I have 125 g of hydroquinone I didn't know what to do with. Thanks a bunch of suggesting this!
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 28-4-2021 at 13:06


I think that's roughly enough for (literally) a ton of styrene.
View user's profile View All Posts By User
njl
National Hazard
****




Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 28-4-2021 at 14:01


Quote: Originally posted by unionised  

Also works with PMMA


Yielding methyl methacrylate?




Reflux condenser?? I barely know her!
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2284
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 29-4-2021 at 03:27


Yup! I think I might have posted a procedure...once upon a time.

[Edited on 29-4-2021 by zed]
View user's profile View All Posts By User
njl
National Hazard
****




Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 29-4-2021 at 04:50


Off topic to this thread, but what did you end up doing with it?




Reflux condenser?? I barely know her!
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 931
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 29-4-2021 at 21:37


Quote: Originally posted by unionised  
I think that's roughly enough for (literally) a ton of styrene.


Had I known (or guessed, rather) that before, I would've added a few mg of it directly to my styrene bottle in the first place.

Talk about late epiphanies… :p
View user's profile View All Posts By User
Swinfi2
Hazard to Others
***




Posts: 131
Registered: 19-2-2018
Location: England
Member Is Offline

Mood: Catalytic

[*] posted on 30-4-2021 at 09:35


I've done this without any catalyst, bloody stinks and it broke my RBF on cooling. Didn't have any inhibitors to keep the product but it worked well enough with minimal thought put into it.

That said if the flask didn't break I probably would never have got it clean from all the charing.
View user's profile View All Posts By User
Keras
National Hazard
****




Posts: 931
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 30-4-2021 at 10:34


Quote: Originally posted by Swinfi2  
I've done this without any catalyst, bloody stinks and it broke my RBF on cooling.


Any idea why it broke?
View user's profile View All Posts By User