Easiest way to make red selenium
Hi. I made red selenium very easily. I used only dilute selenous acid solution and potassium metabisulfite. I mixed solutions and put it in the
sunlight. I think 8 hours is enough to used all selenous acid, because when i added carbonate nothing happened.
I think some of you will use it because metabisulfite is much cheaper than concentrated sulfuric acid and also affordable. Selenium had nice red
colour, but i made it few days ago, since then it has been exposed to sunlight and It therefore has a dark color.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I know of this precedure. You can speed up the procedure by adding some chloride (e.g. dilute HCl). The chloride ions have a catalytic effect on this
reaction.
I have made some of this red Se, cleaned it with distilled water, and dried it. The dry material I put in an ampoule. But unfortunately, the material
is not stable. Over the weeks, the material turns dark grey and half a year later, you hardly can see the red color anymore. The saturation of the
color decreases over time, just to be left with zero saturation, being a dull gray material.
I have seen samples of red selenium for sale, not the amorphous material, made from reduction of a selenite or selenous oxide, but by dissolving the
thus obtained red selenium in some solvent and then very slowly letting the solvent evaporate, so that you get a crystalline solid. These crystals are
dark red and apparently they are more stable. I never purchased some of that red selenium though, because it is very expensive (several euros per
gram), and I still have severe doubts on its long-term stability. I want some for an element collection, stable for years in a display, which is in
daylight.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Does this procedure work with mercury?
:-)
|
|
vano
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline
|
|
Quote: Originally posted by woelen ![](images/xpblue/lastpost.gif) | I know of this precedure. You can speed up the procedure by adding some chloride (e.g. dilute HCl). The chloride ions have a catalytic effect on this
reaction.
I have made some of this red Se, cleaned it with distilled water, and dried it. The dry material I put in an ampoule. But unfortunately, the material
is not stable. Over the weeks, the material turns dark grey and half a year later, you hardly can see the red color anymore. The saturation of the
color decreases over time, just to be left with zero saturation, being a dull gray material.
I have seen samples of red selenium for sale, not the amorphous material, made from reduction of a selenite or selenous oxide, but by dissolving the
thus obtained red selenium in some solvent and then very slowly letting the solvent evaporate, so that you get a crystalline solid. These crystals are
dark red and apparently they are more stable. I never purchased some of that red selenium though, because it is very expensive (several euros per
gram), and I still have severe doubts on its long-term stability. I want some for an element collection, stable for years in a display, which is in
daylight. |
Can you tell me more about chlorine ion catalyst effect?
I agree, every red selenium which i made now have dark colour, but not grey, it has black colour.
|
|
vano
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline
|
|
What do you mean?
|
|
njl
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline
Mood: ambivalent
|
|
I believe unionised is referring to "red mercury" which is (as far as I know) an urban legend stemming from nuclear weapons research.
Reflux condenser?? I barely know her!
|
|
vano
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline
|
|
Oh i understand. Good one
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by njl ![](images/xpblue/lastpost.gif) | I believe unionised is referring to "red mercury" which is (as far as I know) an urban legend stemming from nuclear weapons research.
|
:-)
|
|