Tin Crystals Experiment (video)
Making Tin Crystals: https://www.youtube.com/watch?v=xGVMcYP1fE8
I thought I would post this because it is imho such an amazing, beautiful experiment that very few people seem to know about, or at least publicize.
Ok - I've seen many people talk about using electrolysis to make tin crystals, but this method does not use electrolysis.
I hope you enjoy the video, and try this experiment for yourself. My whole family loves this experiment, and the materials are fairly non-toxic.
As always, any feedback or comments here or on the video are appreciated.
--------------------------------------------------------------
ChemTalk
Chemistry Experiments
[Edited on 3-2-2021 by ChemTalk]
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Nice!
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|