vano
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 14-2-2021 at 11:57
Selenides easy preparation method (?)


Hi. I found some information about synthesis of cobalt selenide.

Copied:
Place the cobalt selenite in a 10% sodium hydroxide solution, stir, drop by drop into the 10% sodium hydroxide solution of sodium thiosulfate , wait until the color of the reaction solution no longer changes, filter after standing, and use water and Wash with 5% hydrochloric acid and dry to obtain CoSe.

My experience:
I tried this. There Also mentioned that it is a yellow solid. When i added Co selenite in NaOH solution it becomes blue, next when i added thiosulfate, solution become clear. And product was dark yellow solid, but is was yellow.

I wonder if it acts similarly on other selenites, for example cadmium selenite.




View user's profile View All Posts By User
vano
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 14-2-2021 at 12:21


It really works. In the case of copper I did everything the same way. Look at copper selenide precipitated. I heated it up 5-10 minutes.

IMG_20210215_001625.jpg - 3.8MB




View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 14-2-2021 at 13:21


How can you be so sure that it is CuSe?

Try the following experiment:
- Dissolve some Na2S2O3 in water.
- In a separate test tube, dissolve some CuSO4 in water.
- Drip the blue solution into the colorless thiosulfate solution --> You get a bright yellow liquid, possibly with some bright yellow precipitate.
- Heat the liquid (or let stand for a long time) --> The yellow material turns black.

The black material is CuS.

So, your material may be CuSe, or CuS, or maybe some mix of both?




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Lion850
National Hazard
****




Posts: 517
Registered: 7-10-2019
Location: Australia
Member Is Offline

Mood: Great

[*] posted on 14-2-2021 at 16:36


Hi Woelen what is the bright yellow product (solution and possible solid) that you mention above? Sounds interesting :)
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2731
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 14-2-2021 at 17:52


This reaction doesn't make sense without stoichiometry. I assume the following reaction is possible:

SeO3(2-) + 6 S2O3(2-) + 6 H+ >> Se(2-) + 3 S4O6(2-) + 6 H2O

But the low activity of hydronium makes it at least implausible, so I think something else must be going on.

This should not be possible:

2 SeO3(2-) + 3 S2O3(2-) + 3 OH(-) >> 2 Se(2-) + 6 SO3(2-) + 3 H(+)

...right? Or maybe it is? Maybe only when there's a transition metal to stabilize Se(2-)?




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
vano
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 14-2-2021 at 23:36


Woelen: i don know if it mixture. In the case of cobalt, it was written that cobalt selenide would be precipitated only. I will try CdSe. If it will be a mixture of yellow sulfide and red selenide I will guess.

Maybe selenide anion is more easy to form then sulfide. I don't know Why they wrote a lie.




View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 15-2-2021 at 00:01


I have written a webpage about the reaction between copper sulfate and sodium thiosulfate, several years ago. The dark solid, which is formed, is CuS, the yellow material most likely is a complex of copper(II) with thiosulfate. It may also be a copper(I) species.

https://woelen.homescience.net/science/chem/riddles/copper+t...




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
vano
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 15-2-2021 at 00:08


I dissolved insoluble selenite dihydrate in hydroxide solution an next i added thiosulfate. I think this reaction is different. Do you have any idea how to test. I think i will add acid and I will observe if red selenium is formed, I will try to measure the mass of this selenium, but it will be too small and may fail.