Author: Subject: Anyone know a source for genuine platinum on titanium electrodes?
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 26-11-2020 at 13:47
Anyone know a source for genuine platinum on titanium electrodes?


I ordered a "platinum on titanium" anode on eBay for my perchlorate cell, but it ran for a few minutes and I discovered it wasn't platinum. It got substantially damaged within minutes. Is there a source for genuine ones at a reasonable price?

Thanks!




Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 26-11-2020 at 15:08


Have a look at this thread
https://www.sciencemadness.org/whisper/viewthread.php?tid=72...

I purchased a titanium electrode and a platinum coated titanium electrode from this ebay seller and was very happy with the product. It has done many weeks of use and is still in top condition.
They do not have Pt electrodes at the moment, but probably worth asking them.
View user's profile View All Posts By User
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 27-11-2020 at 05:14


Thanks for the seller reccomendation. I've messaged them and am yet to hear back. Hopefully they have some



Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 25-1-2021 at 04:56


I am a supplier of platinum group metals: pt,pd,Au,Ag.
I can do very competitive prices. I can't get electrodes
But I can supply thin flatplate (~0.5mm thick flat squares)
which would be good for an electrode. I can also supply
thin wire or rod form.Contact me if you're still
looking for some.