Fluorite
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 133
Registered: 26-12-2018
Location: United Arab Emirates
Member Is Offline
|
|
Calcium carbonate and ammonium nitrate
I tried making calcium nitrate from calcium hydroxide and ammonium Nitrate and and it worked but I have no calcium hydroxide anymore (making calcium
chloride and adding sodium hydroxide is wasteful) so how complicated is it to make calcium nitrate and ammonium carbonate from CaCO3 and NH4NO3?
By the way can copper oxide react with ammonium nitrate/sulfate to make copper nitrate?
And I noticed if this can actually work you can recycle sulfuric acid and make nitric acid without any waste over and over again! But filtering
calcium sulfate is annoying af
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
Quote: | how complicated is it to make calcium nitrate and ammonium carbonate from CaCO3 and NH4NO3? |
calcium carbonate is pretty insoluble and to drive the reaction forward you need to decompose the ammonium carbonate and free ammonia and co2 from
solution, this means you need to heat the solution to boiling or near to boiling, and it will take time, hopefully hours and not days.
i've never tried this reaction tho, maybe using very fine CaCO3 will speed up the reaction considerably
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
B(a)P
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1139
Registered: 29-9-2019
Member Is Offline
Mood: Festive
|
|
I presume you are talking about doing this in an aqueous solution? How are you proposing to dissolve the CaCO3? CaCO3 gets less
soluble in water with increasing temperature.
Quote: Originally posted by Fluorite ![](images/xpblue/lastpost.gif) |
By the way can copper oxide react with ammonium nitrate/sulfate to make copper nitrate?
And I noticed if this can actually work you can recycle sulfuric acid and make nitric acid without any waste over and over again! But filtering
calcium sulfate is annoying af |
I am not sure I follow you here. Do you mean a mixture of ammonium nitrate and sulfate to react with copper oxide? The sulfuric acid formed by
electrolysis can be recycled to make nitric acid?
|
|
Fluorite
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 133
Registered: 26-12-2018
Location: United Arab Emirates
Member Is Offline
|
|
Quote: Originally posted by B(a)P ![](images/xpblue/lastpost.gif) |
I presume you are talking about doing this in an aqueous solution? How are you proposing to dissolve the CaCO3? CaCO3 gets less
soluble in water with increasing temperature.
Quote: Originally posted by Fluorite ![](images/xpblue/lastpost.gif) |
By the way can copper oxide react with ammonium nitrate/sulfate to make copper nitrate?
And I noticed if this can actually work you can recycle sulfuric acid and make nitric acid without any waste over and over again! But filtering
calcium sulfate is annoying af |
I am not sure I follow you here. Do you mean a mixture of ammonium nitrate and sulfate to react with copper oxide? The sulfuric acid formed by
electrolysis can be recycled to make nitric acid? |
I have 2kg mixture of calcium nitrate, calcium ammonium nitrate and ammonium nitrate. I want to turn all these products to nitric acid most
importantly and ammonium hydroxide as cheap as possible, I know adding sulfuric acid to Ca(NO3) can make nitric acid conveniently without distillation
cuz I don't have any glassware expect beakers. And copper can be helpful if I can make copper nitrate or sulfate this can help me because copper
sulfate can be electrolysed to yield sulfuric acid if you have any ideas please do not hesitate
|
|
B(a)P
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1139
Registered: 29-9-2019
Member Is Offline
Mood: Festive
|
|
If you don't have distillation glassware then I see no other way.
It is probably worthy of note that you can acquire the equipment you need to distil HNO3 relatively cheaply, this then opens up a bunch of
routes to HNO3 that would make good use of your calcium ammonium nitrate.
|
|
chornedsnorkack
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 554
Registered: 16-2-2012
Member Is Offline
Mood: No Mood
|
|
Note that ammonium nitrate is actually miscible with water in all proportions.
Seriously. Dry ammonium nitrate melts at 170 Celsius.
Ammonium nitrate melt starts appreciably decomposing above 200 Celsius (to dinitrogen monoxide, mainly).
How liable is ammonium nitrate melt at 170...200 Celsius to react with metal carbonates like calcium carbonate? Removal of both ammonia and carbon
dioxide should drive the reaction ahead.
|
|
B(a)P
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1139
Registered: 29-9-2019
Member Is Offline
Mood: Festive
|
|
Quote: Originally posted by chornedsnorkack ![](images/xpblue/lastpost.gif) | Note that ammonium nitrate is actually miscible with water in all proportions.
Seriously. Dry ammonium nitrate melts at 170 Celsius.
Ammonium nitrate melt starts appreciably decomposing above 200 Celsius (to dinitrogen monoxide, mainly).
How liable is ammonium nitrate melt at 170...200 Celsius to react with metal carbonates like calcium carbonate? Removal of both ammonia and carbon
dioxide should drive the reaction ahead. |
I don't think this will work. Calcium carbonate does not appear to be particularly soluble in molten ammonia nitrate. This is just a patent though,
maybe worth trialing.
https://patents.google.com/patent/US3421878A/en
|
|
Fluorite
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 133
Registered: 26-12-2018
Location: United Arab Emirates
Member Is Offline
|
|
So adding the ammonium nitrate to a sulfuric acid dcm mixture and decanting the dcm layer is the best option right? Ammonium sulfate isn't soluble in
dcm
|
|
B(a)P
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1139
Registered: 29-9-2019
Member Is Offline
Mood: Festive
|
|
Quote: Originally posted by Fluorite ![](images/xpblue/lastpost.gif) | So adding the ammonium nitrate to a sulfuric acid dcm mixture and decanting the dcm layer is the best option right? Ammonium sulfate isn't soluble in
dcm |
I think you are right, I can't see another way.
Is distillation equipment out of the question? Have you asked your secrete santa ?
I do like your commitment to the non-distillation pathway . Best of luck with
it.
|
|