Author: Subject: How to cut 1oz silver bar into pieces that will fit in a test tube
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 30-10-2020 at 06:23
How to cut 1oz silver bar into pieces that will fit in a test tube


So I'm planning to synthesize a handful of silver salts. In anticipation of this, I bought a 1oz bar of silver. If one wanted to cut said bar into approximately 1cm3 pieces, how would one go about that? I've already tried with wire cutters, and while they put a decent dent in the silver, they didn't cut all the way through. I guess the silver is too hard. So how would one cut it? A hacksaw would probably work, but I'd imagine that I'd lose quite a lot of silver doing it they way.

Thanks!




Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4552
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: PhD candidate!

[*] posted on 30-10-2020 at 07:09


Well any silver salt you make is going to necessarily go through silver nitrate as an intermediate, so you might as well toss the entire bar in a beaker and dissolve the whole thing in nitric acid (outside though, as lots of NO2 will be produced too).



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 30-10-2020 at 07:16


That was the plan originally, but the issue is that it'll go through nearly all of my nitric acid to dissolve the whole thing. I guess having to distill some more acid wouldn't be that big of a deal though. I'm already nearly out.



Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
Metallophile
Hazard to Self
**




Posts: 83
Registered: 23-3-2018
Member Is Offline

Mood: No Mood

[*] posted on 30-10-2020 at 07:18


Quote: Originally posted by itsallgoodjames  

A hacksaw would probably work, but I'd imagine that I'd lose quite a lot of silver doing it they way.


Maybe clamp the corner in a vice, and bend it back and forth until it breaks from fatigue?
View user's profile View All Posts By User
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 30-10-2020 at 07:21


That's a great idea. I'll definitely try it. Then I can conserve more of my nitric acid



Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 30-10-2020 at 07:56


Hammer it into a thinner sheet, and then cut with tin-snips.

Even simpler- put as much of your nitric acid as you wish to use for this project into a beaker, add the silver bar.
leave it to react.
When the initial reaction slows down, warm the solution.

The reaction will stop when you run out of acid.
You can remove the remaining silver- probably by pouring off the solution; you might have to filter it.
That will give you silver nitrate solution.

View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2731
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 30-10-2020 at 08:43


Agree with unionised, or at least try hammering it, it allows you to cut more accurately and it's easier to store and weigh metallic silver than any of its salts.
Quote: Originally posted by Texium (zts16)  
Well any silver salt you make is going to necessarily go through silver nitrate as an intermediate, so you might as well toss the entire bar in a beaker and dissolve the whole thing in nitric acid (outside though, as lots of NO2 will be produced too).

If you can obtain methanesulfonic acid, silver methanesulfonate is just as soluble without releasing any toxic gas. Same for trifluoroacetate and probably for ethanesulfonate. In all of these acids you dissolve silver by adding some H2O2.

Silver pyroglutamate is also reported as "soluble in hot water" but no numbers were given in any papers I found. OTC, but speculative. I can find it easily online as a dietary supplement.

[Edited on 30-10-2020 by clearly_not_atara]




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1704
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 30-10-2020 at 08:43


I would try cutting it with a chisel. For softer metals it can be surprisingly effective.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1378
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 30-10-2020 at 08:50


Melt it and pour the molten metal into a large bucket of cold water. It will produce granules of silver, with the size problably depending on a few factors like pouring speed and temperature, but typically they come out about the size of peas.
Its a common method to convert silver into a form thats very convenient for weighing out some amount to use.

[Edited on 30-10-2020 by phlogiston]




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 30-10-2020 at 10:13


Quote: Originally posted by Fulmen  
I would try cutting it with a chisel. For softer metals it can be surprisingly effective.

That was one of the things I was thinking in the beginning, but I'd have to go buy a new chisel, because I accidentally blunted it trying to do that with copper. From what I've read, silver is only a bit softer than copper, so I have a feeling it wouldn't work all that well




Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 30-10-2020 at 10:15


Quote: Originally posted by phlogiston  
Melt it and pour the molten metal into a large bucket of cold water. It will produce granules of silver, with the size problably depending on a few factors like pouring speed and temperature, but typically they come out about the size of peas.
Its a common method to convert silver into a form thats very convenient for weighing out some amount to use.

[Edited on 30-10-2020 by phlogiston]


I would make it into shot, except for I don't have any way to melt it.




Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 30-10-2020 at 10:29


Quote: Originally posted by clearly_not_atara  

If you can obtain methanesulfonic acid, silver methanesulfonate is just as soluble without releasing any toxic gas. Same for trifluoroacetate and probably for ethanesulfonate. In all of these acids you dissolve silver by adding some H2O2.

Silver pyroglutamate is also reported as "soluble in hot water" but no numbers were given in any papers I found. OTC, but speculative. I can find it easily online as a dietary supplement.

[Edited on 30-10-2020 by clearly_not_atara]

The NO2 isn't really all that much of a concern. I've worked with nitric acid numerous times in the past, so an alternative acid isn't really needed. I checked, and all the other ones you mentioned are more expensive per gram than nitric acid, even if I wanted to buy the nitric rather than make it. Plus, a lot of what I want to do with the silver requires it to be the nitrate salt anyways, so it doesn't really make any sense to go with any of those. I'll probably end up flattening it with a hammer and cut it with tin snips or pliers




Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
Clear_horizons_glass
Harmless
*




Posts: 42
Registered: 30-9-2019
Location: Pullman, WA
Member Is Offline

Mood: Glass

[*] posted on 30-10-2020 at 12:04


So I cut silver for giving an iridized affect to glass all the time.
an easier solution I would suggest is to just go out and get a silver coin. Grab one end with some pliers, and beat the other end flat with a hammer on something hard like concrete. Then you can just cut the silver with tin snips without to much effort.

[Edited on 30-10-2020 by Clear_horizons_glass]

[Edited on 30-10-2020 by Clear_horizons_glass]




Clear Horizons Laboratory Glassblowing Services
-------------------------------------------------------------
www.clearhorizonsglass.com
Phone and Fax:
(855) LAB-GLAS
(855) 522-4527
Have a glass project you want made? email me at
info@clearhorizonsglass.com
or message us here |
with a U2U |
message |
\/
View user's profile Visit user's homepage View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2731
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 30-10-2020 at 12:16


Quote: Originally posted by itsallgoodjames  

The NO2 isn't really all that much of a concern. I've worked with nitric acid numerous times in the past, so an alternative acid isn't really needed. I checked, and all the other ones you mentioned are more expensive per gram than nitric acid

I was unaware of your experience, of course. I mention the alternative acids all the time, because I think a lot of people won't even consider silver chemistry for this reason, which is unfortunate because Ag is an entry point to some of the most interesting chemistry that is accessible with minimal equipment -- obviously photography, but also lots of other stuff.

Pyroglutamic acid is apparently available as a dietary supplement, so maybe I can make my own data about how well it works.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 30-10-2020 at 12:31


Unless carefull and used to them you are going to have small losses by the chemical processes. Also, it involves waste management.
The hackswaw method isnt that bad and it avoids a lot of efforts. You might also lose some silver here but with a piece of paper under the vice you should get most of it. I use the hacksaw to cut pieces I can put through the neck of my reactor so I'm certain all the nitric acid is used up.

In both cases you'll probably lose a bit but still will have probably more than 30 grams to experiment with including losses.

You seem to have only a little bit of acid left. Cut, bend, tear, flatten if you can and then use your acid. Go for a beaker if your samples are above 1-2 grams

Next time get a one ounce COIN :D




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 30-10-2020 at 13:24


The trouble with a hacksaw is iron contamination- especially of the "sawdust", if you plan to catch + re-use it.

I guess an HCl wash of the metal would strip Fe but leave Ag behind.

But I still think the easy "solution" is to put the metal in a beaker with however much nitric you want to "spare" for this purpose, and let it react.

Incidentally, does adding H2O2 to HNO3 work?
Does the NOx get oxidised back to HNO3?
View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 30-10-2020 at 13:32


Quote: Originally posted by unionised  


Incidentally, does adding H2O2 to HNO3 work?
Does the NOx get oxidised back to HNO3?


I will give it a try later today and report back.


[Edited on 30-10-2020 by B(a)P]

In a flask1 g of silver was added to 2 mls dH2O and 2 mls HNO3 70%
In a beaker (that is all I had) 1 g of silver was added to 2 mls 35% H2O2 and 2 mls HNO3 70%

Very little happened at room temp, but upon heating both vessels were visibly reacting and no NO2 was visible from the vessel with peroxide.

I will check yields tomorrow and report back.

Next test might be to add more silver than the acid can dissolve and see which mix results in less silver.

[Edited on 31-10-2020 by B(a)P]

Sorry this post got a bit screwed up because of a passing lighting storm. Here is the comparison with a little heat.

[Edited on 31-10-2020 by B(a)P]

IMG_20201031_195922.jpg - 4.7MB

[Edited on 31-10-2020 by B(a)P]
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1704
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 30-10-2020 at 14:14


Quote: Originally posted by itsallgoodjames  
silver is only a bit softer than copper


There might be some language issues at play here. I was thinking of a stone chisel, not a wood chisel.

I discovered this while making some metal strips from stainless steel pipe (only suitable stock i had). Hacksaws don't really cut well in soft stainless, so I ended up parting rings of steel tubing and then split them using a stone chisel before hammering them down into flat strips. It's surprisingly effective on softer metals.




We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
itsallgoodjames
Hazard to Others
***




Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline


[*] posted on 30-10-2020 at 19:08


I think I'm going to hammer it reasonably thin, then cut it with tin snips. Next time I'll buy some silver shot on eBay and save all the effort. No clue why I didn't do that beforehand, given I generally purchase metals in the form of turnings or powder. Not like that'll be any time soon though, as I usually work on very small scales (less than a gram) for most things, due to cost, among other reasons. That's why I was asking about using a test tube, rather than a beaker. Anyways, thanks for the help



Nuclear physics is neat. It's a shame it's so regulated...

Now that I think about it, that's probably a good thing. Still annoying though.
View user's profile View All Posts By User
TriiodideFrog
Hazard to Others
***




Posts: 108
Registered: 27-9-2020
Member Is Offline


[*] posted on 30-10-2020 at 23:21


You could melt the silver and try to pour it into a quartz test tube. If you have to get the silver back out, you can just sacrifice the test tube.
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 30-10-2020 at 23:33


Bolt cutters Will take a chunk out of it.

[Edited on 31-10-2020 by symboom]
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6269
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 31-10-2020 at 02:50


Quote: Originally posted by TriiodideFrog  
You could melt the silver and try to pour it into a quartz test tube. If you have to get the silver back out, you can just sacrifice the test tube.

This would seem to be the worst of the suggestions so far. The prece difference between silver and quartz glassware would make this prohibitive.

I would think dissolving what you need in HNO3 as you need it would make the most sense.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 31-10-2020 at 03:07


Quote: Originally posted by TriiodideFrog  
You could melt the silver and try to pour it into a quartz test tube. If you have to get the silver back out, you can just sacrifice the test tube.

You could.

You could take your clothes off and run round naked.
It also wouldn't help.

It would have the advantage that you wouldn't need to waste money on a quartz tube and even more so, it wouldn't raise the problem of melting the silver - which the OP said he couldn't do.
"
I would make it into shot, except for I don't have any way to melt it."
View user's profile View All Posts By User
Fyndium
International Hazard
*****




Posts: 1192
Registered: 12-7-2020
Location: Not in USA
Member Is Offline


[*] posted on 31-10-2020 at 08:11


Never cut any precious metals with sawing or grinding tools. You will lose a huge amount, even if you try to collect the dust.

Get bigger cutters, or borrow bolt cutters.
Try cold chiseling it in a vise.
Put it in a drill press, drill it with clean and sharp bit with low rpm and collect the turnings.
Cast it into round bar and turn it in a lathe for more turnings.

I used to squeeze metal into thinner form with 50 ton hydraulic press. Use smaller mandrels to get more pressure per area, with 10mm square HSS bars I can form pretty much any metal, including non-hardened steel. If you've got even more access, you can turn a drawing mandrel and just press the metal into a wire of desired diameter.
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2281
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 31-10-2020 at 08:17


Easy. Just make some more Nitric Acid.

Or, employ a jewelers saw, to cut uo your bar. Hold it over a beaker, to catch any filings.

Owning a jewelers saw, is very handy. The hair-like blades are inexpensive, sharp and efficient.

https://www.ebay.com/itm/GERMAN-STYLE-SAW-FRAME-JEWELERS-SAW...

[Edited on 31-10-2020 by zed]
View user's profile View All Posts By User
 Pages:  1  

  Go To Top