Thermometers: alcoholic vs. Hg filling
I just dropped my last glass thermometer I used for almost everything.
I was about to order some glass stuff from a laboratory shop anyway.
Now they have two types:
One has an alcohol based filling, one has mercury.
The alcoholic version is said to be "fully submerging", the mercury version has a minimum dept of 70mm.
Since the mercury version is only slightly more expensive and seems to be superior - that would be my choice.
Any objections?
What would you prefer and why?
Measuring a liquid in a small beaker with 30mm filling height with a 300mm thermometer that should be fully submerged will lead to errors, I'm aware
of the situation. However, do you have some experience about the extent of error one can expect? For some 60°C in the beaker, 18°C air, no wind, or
some other example situation you can think of?
My question here is, what amount of error would
|
|
teodor
National Hazard
  
Posts: 981
Registered: 28-6-2019
Location: Netherlands
Member Is Offline
|
|
Is it ever dependent on the filling type? I have not Hg thermometer with the scale up to 250C but on 131 (iso-amyl alcohol boiling temp) the error is
already 8 degrees when the submerged part is equal to the mark 90-100C. On 100 it is 3 degrees but below 90 (in the submerged part) there is no error.
On the other hand I have a thermometer with NS14/23 ground glass joint (so, the submerge point is constant) and it doesn't require correction.
So, I think it is not dependent on Hg/alcoholic/anything.
[Edited on 27-10-2020 by teodor]
[Edited on 27-10-2020 by teodor]
|
|
DraconicAcid
International Hazard
   
Posts: 4405
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Online
Mood: Semi-victorious.
|
|
I figure the alcohol one is going to be less hassle to clean up when I eventually break it.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Herr Haber
International Hazard
   
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
I bet one is jacketed with the writings inside and the other one is not and has the writings outside.
One you can put in a beaker full of acid, the other one will lose all it's writing and should be kept for distillations.
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
valeg96
Hazard to Others
 
Posts: 254
Registered: 6-4-2014
Location: Italy
Member Is Offline
Mood: Moodless
|
|
I have plenty of vintage Hg thermometers found at a flea market for 1€/each, but out of curiosity I've also purchased a bunch of those cheap Hg lab
ones you can find on aliexpress.
They seem to be pretty accurate (±1°C, you can tell while distilling stuff), though they can develop bubbles if improperly used. If you have a very
small budget consider purchasing those.
|
|
itsallgoodjames
Hazard to Others
 
Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline
|
|
I use alcohol ones for this exact reason. I tend to break a lot of thermometers, and mercury ones are a pain to deal with if you
break them. If you're at all likely to break it, go with the alcohol one. They're so much easier to clean up
Nuclear physics is neat. It's a shame it's so regulated...
Now that I think about it, that's probably a good thing. Still annoying though.
|
|
Mateo_swe
National Hazard
  
Posts: 550
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
What about the very cheap Type K Thermocouples that come with a small display.
Are those not accurate enough?
If one put the sensor in a glasstube sealed in one end they would have about the same diameter as a normal lab thermometer.
|
|
itsallgoodjames
Hazard to Others
 
Posts: 276
Registered: 31-8-2020
Location: America Lite
Member Is Offline
|
|
Quote: Originally posted by Mateo_swe  | What about the very cheap Type K Thermocouples that come with a small display.
Are those not accurate enough?
If one put the sensor in a glasstube sealed in one end they would have about the same diameter as a normal lab thermometer.
|
I've been planning to switch to one of those for a while now, I've heard some pretty good things about them. Plus you can hook them up to an Arduino
to monitor your reactions which would be nice.
Nuclear physics is neat. It's a shame it's so regulated...
Now that I think about it, that's probably a good thing. Still annoying though.
|
|
Dr.Bob
International Hazard
   
Posts: 2804
Registered: 26-1-2011
Location: USA - NC
Member Is Offline
Mood: Mildly disgruntled scientist
|
|
Mercury ones are better on wide ranges of temps. Alcohol ones can do lower temps better, and are safer and easier to ship. Just depends on what you
want to do. I use both, but mostly non-Hg ones at work. If people in the US need therms, I still have a few of both types, in several ranges and
types. But too hard to ship overseas, due to many regs. Even in the US, Hg ones can only be shipped by FedEx easily.
|
|
dangerous amateur
Hazard to Others
 
Posts: 148
Registered: 8-7-2011
Member Is Offline
Mood: No Mood
|
|
Thanks.
Quote: |
I bet one is jacketed with the writings inside and the other one is not and has the writings outside. One you can put in a beaker full of acid, the
other one will lose all it's writing and should be kept for distillations. |
I think the scale is inside the thermometer.
I once had one with the number on the outside and yes, the once in acid the paint was gone
I'll go for mercury. I dont plan to break it
On the long run a thermocouple would be more useful, but I postponed that.