How violent is the reaction between ammonia and cs2? I want some thiocyanates to try the fake blood experiment
|
|
metalresearcher
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 737
Registered: 7-9-2010
Member Is Offline
Mood: Reactive
|
|
I tried it this morning by putting S + C powder in a stainless steel retort placed in a 900 C electric furnace and the end in a test tube cooled by
water. But I was stupid. I saw all sulfur condensing in the test tube and I realized that this was way beyond the boiling point of S (445 C), so it
did not have the time to react with the C(harcoal powder).
Carefully smell tests on the test tube gave hints to tiny amounts of CS2, but really very small, because almost all vaporized off unreacted.
I have to make a separate heater to vaporize the S and lead that over C heated to 900 C.
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 771
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
Quote: Originally posted by metalresearcher ![](images/xpblue/lastpost.gif) | I tried it this morning by putting S + C powder in a stainless steel retort placed in a 900 C electric furnace and the end in a test tube cooled by
water. But I was stupid. I saw all sulfur condensing in the test tube and I realized that this was way beyond the boiling point of S (445 C), so it
did not have the time to react with the C(harcoal powder).
Carefully smell tests on the test tube gave hints to tiny amounts of CS2, but really very small, because almost all vaporized off unreacted.
I have to make a separate heater to vaporize the S and lead that over C heated to 900 C.
|
I guess the stainless will react with sulphur vapor particularly at 1000C
How did the stainless steel react to the sulphur vapour ?
I have assumed the carbon needs to be in lump form and the reactor sufficiently tall and only heated at the base with the upper part of the reactor
below the boiling point of sulphur and therefore acting as reflux for the sulphur while letting the low boiling CS2 pass.
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
rockyit98
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline
Mood: no mood is a good mood
|
|
Pyrite and charcoal can be heated together at 700C or higher to make CS2 without elemental sulfur. apparently that's how it was first produced, but I
don't know about the yield or what are the side products.