Author: Subject: Leaded glass in light bulbs
wg48temp9
National Hazard
****




Posts: 782
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 12-10-2020 at 18:08
Leaded glass in light bulbs


I have examined the glass to metal seals and evacuation tubes of various light bulb. I have also worked the glass in a reducing flame but neither my working or the manufacturer has left the metallic gray black discoloration typical of leaded soda glass.

I suspected the glass does not contain significant amounts of lead. So I checked. Apparently the Europe Union banned leaded glass in light bulbs in 2011. See Attachment: leaded-glass-S1878029612006184.htm (80kB)
This file has been downloaded 317 times

That's good news if you are in Europe and you want to work old fluorescent tubes with the cheap torches that have reducing flames. The bad news is the higher softening temperature requires a hotter flame.

On a different point from that paper "Leaded fluorescent lamp glass can also be divided into three types according to PbO concentration as
light red lead, medium red lead, heavy red lead, which is 11%, 20%, and above 28% PbO respectively" No wounder it goes black in a reducing flame.






I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
Clear_horizons_glass
Harmless
*




Posts: 42
Registered: 30-9-2019
Location: Pullman, WA
Member Is Offline

Mood: Glass

[*] posted on 13-10-2020 at 10:45


So in your experience lead glass require a much more oxidizing flame to not develop the dark discoloration?



Clear Horizons Laboratory Glassblowing Services
-------------------------------------------------------------
www.clearhorizonsglass.com
Phone and Fax:
(855) LAB-GLAS
(855) 522-4527
Have a glass project you want made? email me at
info@clearhorizonsglass.com
or message us here |
with a U2U |
message |
\/
View user's profile Visit user's homepage View All Posts By User
wg48temp9
National Hazard
****




Posts: 782
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 13-10-2020 at 14:04


Quote: Originally posted by Clear_horizons_glass  
So in your experience lead glass require a much more oxidizing flame to not develop the dark discoloration?


My experience is that a reducing flame reduces the lead in glass to lead metal. I would assume a neutral or an oxidising flame would not reduce the lead to metal. I can not confirm that by my direct experience because I have never worked glass containing lead with a neutral or oxidising flame. Though I have read that that is the case.





I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User

  Go To Top