Author: Subject: H2O2 use in the oxidization of Cu for the synthesis of TACN
foreign maple
Harmless
*




Posts: 26
Registered: 14-12-2017
Location: Somewhere up north
Member Is Offline

Mood: I'm fine

smile.gif posted on 10-9-2020 at 10:35
H2O2 use in the oxidization of Cu for the synthesis of TACN


hello i was wondering if it would be possible to use H2O2 to substitute the introduction of O when synthesizing TACN. i know you usually use it when forming other Cu salts like Copper Chloride.

Has anyone ever thought of this idea and put it in practice?
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1246
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 10-9-2020 at 18:00


Why? Just use copper nitrate. If you don't have any, dissolve some copper wire in nitric acid.



View user's profile View All Posts By User
foreign maple
Harmless
*




Posts: 26
Registered: 14-12-2017
Location: Somewhere up north
Member Is Offline

Mood: I'm fine

[*] posted on 11-9-2020 at 06:24


Quote: Originally posted by Bedlasky  
Why? Just use copper nitrate. If you don't have any, dissolve some copper wire in nitric acid.


true i was just wondering if this process would work. there are much more efficient methods such as using copper nitrate or using CuO but ia just interested if H2O2 would to oxidize the Cu.
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 11-9-2020 at 06:48


You might end up making copper peroxide depending on temperature and peroxide also destroys ammonium hydroxide
If you have copper powder ammonium hydroxide.

Yes it will work
just not as efficient as HCl and hydrogen peroxide it also takes a bit of time if you are using copper wire which has less surface area copper powder would work even better but you would have a copper salt like copper sulfate to make that anyways.

[Edited on 11-9-2020 by symboom]




View user's profile View All Posts By User
njl
National Hazard
****




Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline

Mood: ambivalent

[*] posted on 11-9-2020 at 06:54


By TACN do you mean tetraamine copper nitrate?
View user's profile View All Posts By User
foreign maple
Harmless
*




Posts: 26
Registered: 14-12-2017
Location: Somewhere up north
Member Is Offline

Mood: I'm fine

[*] posted on 11-9-2020 at 08:46


Quote: Originally posted by njl  
By TACN do you mean tetraamine copper nitrate?
yes i do
View user's profile View All Posts By User
foreign maple
Harmless
*




Posts: 26
Registered: 14-12-2017
Location: Somewhere up north
Member Is Offline

Mood: I'm fine

[*] posted on 11-9-2020 at 08:50


Quote: Originally posted by symboom  
You might end up making copper peroxide depending on temperature and peroxide also destroys ammonium hydroxide
If you have copper powder ammonium hydroxide.

Yes it will work
just not as efficient as HCl and hydrogen peroxide it also takes a bit of time if you are using copper wire which has less surface area copper powder would work even better but you would have a copper salt like copper sulfate to make that anyways.

[Edited on 11-9-2020 by symboom]

Thanks! yeah that would make sense about forming copper peroxide. I forgot about the peroxide degrading the NH4OH i will definitely make some copper powder in the near future.

[Edited on 11-9-2020 by foreign maple]
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 11-9-2020 at 11:31


Also heating up copper pipe or copper wire till it turns black will make copper oxide on the surface and when it cools it flakes off so no sanding needed. This could be used to dissolve copper into ammonium hydroxide forming tetramine copper hydroxide