Activated carbon extraction?
https://www.youtube.com/watch?v=son8yyD-T_E
Could activated carbon be used to absorb dissolved compound from a solution and vacuum distill it off? Considering the solvent is of low molecular
weight and the desired compound a high mw?
https://www.jstage.jst.go.jp/article/tanso/2015/269/2015_140...
[Edited on 28-7-2020 by Fyndium]
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3027
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
I don't think so. As far as I know there is no way to reactivate activated carbon besides heating beyond the point where the absorbed compounds
decompose.
|
|
Fyndium
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1192
Registered: 12-7-2020
Location: Not in USA
Member Is Offline
|
|
I doubt that. I have used activated carbon to clean alcohol and when boiled and finally dried in oven, it releases a lot of smelly vapors. The odor
evolution pretty much ceases above 200C after some time, indicating all the compounds it has adsorbed are of lower bp than that. I expect that
everything that boils off rather than decomposes, will boil at some point, in a vacuum much more so, and what eventually decomposes, will gradually be
reduced until only carbon and non-volatile elements are left.
Silica and carbon are aDsorbents, not absorbents, as far as I know the difference, and the molecules are practically glued or grabbed to their surface
instead of dissolving into the crystal lattice (like carbon does to steel, or hydrogen to palladium, etc) and will be released when the energy to
vapor pressure ratio grows large enough.
The key concept here was to adsorb a compound dissolved in a large amount of solvent to be filtered in a concentrated form which is a lot easier to
distill off rather than evaporating the entire solvent first because carbon is passive, low energy element which does not boil or melt and hence only
the residual solvent and the target compound need to be evaporated.
[Edited on 28-7-2020 by Fyndium]
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3027
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
I guess the carbon you cleaned the alcohol with was moist with alcohol when you oven dried it? In that case there was a lot more alcohol than just the
alcohol it adsorded.
It would be interesting to see if it still smells when you first air dry the carbon and then put in an oven.
|
|
Fyndium
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1192
Registered: 12-7-2020
Location: Not in USA
Member Is Offline
|
|
The carbon was first washed and then boiled in water for half an hour prior to oven and that should get rid of most of the lower boiling compounds.
The smell was not ethanolic at all, but most likely fusel oils and other junk, the smell is difficult to describe, but it's remotely sweetish or
aromatic to say.
This was done to alcohol that was first stripped to 60% abv and then fractionated at 78.2C into foreshots, heads, hearts and tails and measured 95%
with abv meter at ntp.
|
|
DavidJR
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline
Mood: Tired
|
|
Thermal desorption cartridges containing activated carbon are routinely used for analysis of VOCs in atmospeheric air.
|
|
macckone
Dispenser of practical lab wisdom
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Short answer is yes, activated carbon can and is used for separating compounds.
Better answer is use column chromatography separation,
silica is often used as the stationary phase and is easier to work with.
Numerous other stationary phases are possible with activated carbon being one of the hardest as it has to be heated to release the compounds
effectively. The heat required varies by compound which provides a good way to separate the adsorbed compounds.
|
|