High temperature pipe wrapping that is non conductive (electrically)


I need to wrap a small pipe (1/4" - 1/2" diam) so I can wrap nichrome wire around it so I can keep the temp high on the piping. The minimum operating temp will be 680F but will probably be operating at 1000F or so and ideally there would be some safety margin above that.

I've found some fiberglass sleeving that is suitable but it's only available in 50-100ft sections and is too expensive considering I need 1-2ft. I found suppliers in China (ebay listing) but with shipping times now, that is no where near ideal. I'm wondering if anyone knows of any businesses that would use this stuff in their daily business from electricians, HVAC, or automotive applications. I was hoping to I might be able to find a business that uses it and maybe buy a small piece.

Here are some sites that are bulk suppliers and it shows some of the applications. It looks like the sleeves are often used to insulate compressor or oil lines in vehicles or HVAC

https://www.techflex.com/high-temperature

https://www.cabletiesandmore.com/high-temperature-braided-sl...

If anyone is interested in ordering some smaller quantites, this seller has all different sizes and sells them in meter lots but it is shipped from china.

https://www.ebay.com/itm/1-40mm-White-600-C-HIGH-TEMP-Fiberg...

[Edited on 7-16-2020 by RogueRose]
View user's profile View All Posts By User
mysteriusbhoice
Hazard to Others
***




Posts: 477
Registered: 27-1-2016
Member Is Offline

Mood: Became chemistry catboy Vtuber Nyaa

[*] posted on 16-7-2020 at 09:41


try some KAO-WOOL pipe sleaves
https://www.morganthermalceramics.com/en-gb/products/high-te...
a bit fluffy but it should do the job!
View user's profile Visit user's homepage View All Posts By User
Junk_Enginerd
Hazard to Others
***




Posts: 250
Registered: 26-5-2019
Location: Sweden
Member Is Offline


[*] posted on 17-7-2020 at 02:07


This can't possibly be an issue to find. You can buy fibreglass mats used for composite plastics in almost any hardware store. Then just cut them to size. Same hardware stores are likely to also have strips of fibreglass which have seams on the edges, this is nice since you don't have to deal with all the fraying you get with cut edges. Seriously that fraying drives you nuts and suddenly everything looks like its been tarred and feathered unless you're careful.

It is also not too uncommon to wrap motorcycle or car exhausts with some form of fibreglass for heat retention, I assume many automotive/tuning shops will have these in stock.

Fibreglass sleeves of smaller dimension should also be available from electronics suppliers like digikey.

If necessary, the fibreglass could be fixated with sodium silicate, or a paste of sodium silicate and an inert ballast like clay, sand or something similar.

[Edited on 17-7-2020 by Junk_Enginerd]
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 769
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 17-7-2020 at 03:27


The problem is the maximum operating temperature of most thermal insulation is not necessarily its operating temperature as an electrical insulation

Glasses in particular tend to have significant electrical conductivity at elevated temperature so most cannot be used for electrical insulation at 500C.

[Edited on 7/17/2020 by wg48temp9]




I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 17-7-2020 at 13:38


Ceramic fiber paper



"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
Texium
Administrator
Thread Moved
29-11-2023 at 13:33

  Go To Top