Removal of superfine copper particles from stir bar


Today I got some superfine copper particles stuck in the Teflon coating of the stir bar and it doesn't go off by a paper towel or scratching, and I have no nitric acid.

Is there any other way to remove them?




Collected elements:
Al, Cu, Ga, C (coal), S, Zn, Na

Collected compounds:

Inorganic:
NaOH; NaHCO3; MnCl2; MnCO3; CuSO4; FeSO4; aq. 30-33% HCl; aq. NaClO; aq. 9,5% ammonia; aq. 94-96% H2SO4; aq. 3% H2O2

Organic:
citric acid, sodium acetate, sodium citrate, petroleum, mineral oil
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 1-7-2020 at 16:41


Quote: Originally posted by Draeger  
Today I got some superfine copper particles stuck in the Teflon coating of the stir bar and it doesn't go off by a paper towel or scratching, and I have no nitric acid.

Is there any other way to remove them?


acetic acid + H2O2
HCl + H2O2
H2SO4 + H2O2

any acid and an oxidizer pretty much





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
Draeger
Hazard to Others
***




Posts: 185
Registered: 31-1-2020
Location: North-Rhine Westfalia, Germany
Member Is Offline

Mood: Slowly getting ready for new projects

[*] posted on 1-7-2020 at 17:03


Quote: Originally posted by Ubya  
Quote: Originally posted by Draeger  
Today I got some superfine copper particles stuck in the Teflon coating of the stir bar and it doesn't go off by a paper towel or scratching, and I have no nitric acid.

Is there any other way to remove them?


acetic acid + H2O2
HCl + H2O2
H2SO4 + H2O2

any acid and an oxidizer pretty much

Oh wow, didn't think it'd be that easy. Thanks.

I know what the other two reaction products with H2O2 are, but what does acetic acid and H2O2 make?




Collected elements:
Al, Cu, Ga, C (coal), S, Zn, Na

Collected compounds:

Inorganic:
NaOH; NaHCO3; MnCl2; MnCO3; CuSO4; FeSO4; aq. 30-33% HCl; aq. NaClO; aq. 9,5% ammonia; aq. 94-96% H2SO4; aq. 3% H2O2

Organic:
citric acid, sodium acetate, sodium citrate, petroleum, mineral oil
View user's profile View All Posts By User
Syn the Sizer
National Hazard
****




Posts: 591
Registered: 12-11-2019
Location: Canada
Member Is Offline


[*] posted on 1-7-2020 at 18:22


I believe it is just a solution of H2O2 and acetic acid. The H2O2 helps produce an oxide layer for the acid to attack.

[Edited on 2-7-2020 by Syn the Sizer]
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 1-7-2020 at 22:27


Everyone is forgetting ammonia and air by shaking them in solution to make them soluble in ammonia as a complex nice and cheapest.