Cuting cerium metal
Hi.
I have small piece of cerium metal (3g). I read that cerium is soft metal which can be cut by knife. But this isn't truth. I tried it and it didn't
work.
I want to try cut few small pieces of cerium and dissolve them in different acids.
Have you any experiences or ideas how cut it?
|
|
Heavy Walter
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 127
Registered: 17-12-2015
Location: Argentina
Member Is Offline
Mood: No Mood
|
|
Hi
In Mohs´s scale is 2.5 so it is not too hard.
Depening on the shape you can use a cutting plier.
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
Or just a file ?
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6252
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
If you use an angle grinder, prepare for sparks.
I have a 1.1kg ingot. I am not planning on cutting it at all. When I get into Ce chemistry it will likely be via CeO2 or purpose bought pellets.
|
|
diddi
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
i made a tool from an 8.8 HT bolt which i use as a chisel in a press for cutting (shearing) metals. no sparks and good control. angle grinder blades
get shredded by many metals and there is a lot of wastage esp if the sample is small
Beginning construction of periodic table display
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
If it's only 3 grams you could also just fold a paper around it and hammer it a few times.
Somewhere around I have several blocks of Cerium mixed with a bunch of other lanthanides. I bought them from a pyro store but they were all little
pyramids at some point. The base was irregular as if it had been broken off a mold or probably sintered.
I remember researching what were their original purpose (never heard of Cerium in pyro unless you count the lighter!) could have been. They are
probably used in foundry to add trace lanthanides in some exotic alloys.
Anyway, the last time I found them I made a mess of oxides. I shouldnt have left them in their plastic bag...
@jsum1 The angle grinder could be fun but I thought I could find myself a very tall bridge or tower, heat one of my blocks with a blowtorch and drop
it
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6252
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
I was not serious about using an angle grinder. But it would be spectacular.
If I was to cit the piece I have, I would probably use a hacksaw and collect the filings for making a cerium salt.
|
|
Bedlasky
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1225
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline
Mood: Volatile
|
|
Thanks for suggestions.
Cutting plier is good choice. I tried it today and it's good for cutting small pieces of metal, which is good for test tube scale reactions.
|
|