Ruthenium too good to be true?
https://www.ebay.co.uk/itm/RUTHENIUM-ALLOY-Powder-35g-Very-H...
35g Ru powder for just £22? Seems too good to be true...
|
|
clearly_not_atara
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2732
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
Ru is by far the cheapest of the platinum group metals. This price seems low, but not entirely out of the question
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
plus it says ALLOY, alloyed with what and in what percentage it's not specified, it could be 90% or 10%, and givem the price, i think it's on the low
side
[Edited on 4-12-2019 by Ubya]
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 774
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
It does not say how much Ru is in the alloy or what the other elements are?
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
fff
Harmless
Posts: 22
Registered: 20-12-2018
Location: UK
Member Is Offline
|
|
Same thing with slightly different mass, but also mentioned it's 99.99%...
https://www.ebay.co.uk/itm/RUTHENIUM-Alloy-Powder-45g-Very-H...
|
|
stoichiometric_steve
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 827
Registered: 14-12-2005
Member Is Offline
Mood: satyric
|
|
It's 99.99% powder, the remainder being not powder. So pretty pure powder.
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
99.99% pure alloy
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Just checked the price for ya, Ru is currently $250 or GBP190/ozt. So that does sound suspicious to me, and I doubt it will be 99.99% Ru. If you do
want to buy it, proceed with caution and don't expect it to be 99.99% Ru. If it turns out really is, then congrats.
|
|
Mateo_swe
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 528
Registered: 24-8-2019
Location: Within EU
Member Is Offline
|
|
As it clearly says it´s an alloy (a mix), so it´s not pure Ru.
If interested to buy this one should ask the seller what alloy and the %.
|
|
diddi
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
then what do you do with an alloy? not much good as an element sample, not much good as an Ru source if it is loaded with some unknown contaminant
that may be difficult to remove...
not much good at all imo
Beginning construction of periodic table display
|
|
Fleaker
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1252
Registered: 19-6-2005
Member Is Offline
Mood: nucleophilic
|
|
Looks like RuO2 to me.
Most commercial Ru metal (sponge) is a light grey powder like the rest of them (barring osmium, that's blue).
Neither flask nor beaker.
"Kid, you don't even know just what you don't know. "
--The Dark Lord Sauron
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5111
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
I wasn't very interested in ruthenium, so I didn't bother much with this thread at the outset.
But I just looked at teh ebay link.
I have "dealt" with that seller before.
Sometimes I got what I paid for.
Sometimes I did not get what I paid for- the material was not "as described".
Proceed with caution + test before you give feedback.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7998
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
With this seller you can have good look, but you also can have something completely different.
I have purchased quite a few interesting chemicals from him. To name a few:
- V2O5 --> very good quality material, dissolves completely clear in a solution of NaOH.
- MnO2 --> questionable stuff. Contains a lot of iron. Good enough for energetic thermite-like reactions, but not for anything else.
- NH4ReO4 --> the real thing! pure stuff. I obtained 160 grams for just GBP 40.
- Ru(OH)3 --> not Ru(OH)3, but hydrous RuO2. But it only contains Ru as a metal. A good buy, GBP 20 for 70 grams.
- MoO3 --> impure stuff, contains a lot of brown stuff, does not dissolve completely in solution of NaOH
- WO3 --> very good quality stuff, pure sulphur-yellow material.
- Re --> something completely different, the metal does not dissolve in any acid I have, while Re dissolves in HNO3. With the latter, I received a