Granulation of glass and fine abrasive powder


Hey guys,

I ran in some trouble with my current project. The given task is to improve the flowability of very fine powder. Therefore, I was given a very fine glass powder (~5µm) and an abrasive powder (silicon carbide, ~15µm) and my goal was to granulate these two into a powder with a fine share as little as possible.

I have tried several methods, of which most are based on Heatgranulation.

My ideas are the following:

-sol-gel process via sodium silicate (reaction with the glass?!)

-Heatgranulation with an organic binder (which is burned after the granulation)

-Creating a very hard solid mass and crushing it down to the right size

Do you guys have any idea on how to granulate the given powders (without using industrial-sized apparatus like freeze-drying or spray drying)

Thank you in advance :)
View user's profile View All Posts By User
draculic acid69
International Hazard
*****




Posts: 1371
Registered: 2-8-2018
Member Is Offline


[*] posted on 7-11-2019 at 04:28


Ball mill. Blender
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 7-11-2019 at 14:07


Definitely a job for a ball mill. Cheap and easy way to do it is a rock tumbler and some steel slingshot ammo (or other steel spheres).



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 786
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 8-11-2019 at 00:26


If by granulation you mean to form the mixture in to +millimeter sized chunks you could use the method used by amiture gun powder makers:

The mixture with binder is forced thru a perforated zinc sheet. When dry its shaken or tumbled briefly to break up loosely sticking granulations then sieved to obtain the correctly sized granulation. The dust and large bits are recycled back in to the next batch. There is probably a youtube video demonstrating the method.

The method is useful for pelletizing almost anything provided a suitable binder is available.

Think about how a meat grinder works, some extrude and cut.





I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
Praxichys
International Hazard
*****




Posts: 1063
Registered: 31-7-2013
Location: Detroit, Michigan, USA
Member Is Offline

Mood: Coprecipitated

[*] posted on 11-11-2019 at 07:02


For more info, that process was known as corning.

https://en.wikipedia.org/wiki/Gunpowder#Corning
View user's profile Visit user's homepage View All Posts By User