silicon carbide from old abrasive paper ("sand" paper)
i been keeping/collecting used abrasive paper for a while. lately i needed SiC fine powder to mix with fire clay (70%Al2O3 30%SiO2) to increase its
thermal conductivity,since SiC have high value about upward of 200W m−1K−1.since SiC is very hard i can't ball mill it.so i turned to my old
collection of abrasive paper.
some are black and others are not. only black ones are made of SiC. rest are Al2O3.so i cut a sample of black ones and measured it weigh using a
milligram scale .then burned it heating it to red hot to burn off carbon then measured the residue .after some calculation it was 60% SiC.i was so
happy .
i desired 200g of SiC so burned all of my old black abrasive paper.
i washed the SiC and let them dry.used a strainer to get the fine SiC.
the image below is a new abrasive paper and the rest after the straining since i used the good stuff.sorry![:(](./images/smilies/sad.gif)
hope this helped. thank you.
FYI:you can use SiC and fire clay to make Microwave crucible because SiC absorbs Microwave well.can get up to 1500C if you used proper clay and
insulation.
"A mind is a terrible thing to lose"-Meisner
|
|
Boffis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1851
Registered: 1-5-2011
Member Is Offline
Mood: No Mood
|
|
Can't you just buy the silicon carbide? I use it for polishing rock slabs and its dirt cheap. You can even buy it ready ground from 32 to 1200 mesh,
its available in 100 to 500g amounts on ebay what more could you want?
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
The satisfaction of doing it yourself.
The joy of knowing it is recycled.
|
|
Ubya
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline
Mood: I'm a maddo scientisto!!!
|
|
how do they mill it industrially?
i have a big clump of SiC crystals, i'd like to grind some to make abrasive powder
---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
|
|
fusso
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Sometimes extracting the treasury parts from some trashy bois is satisfying and therapeutic, and they're free too!
|
|