a11051605
Harmless
*




Posts: 21
Registered: 25-8-2017
Member Is Offline

Mood: No Mood

[*] posted on 14-9-2019 at 18:08
Home made Flocculant for Lye solution and hydroxides?


Was wondering if any one had a good flocculant to use in a lye solution. I know their are brand name flocculants you can buy off the shelf but was wondering if any one could recommend a decent flocculant that you can make at home? Iv seen mention of aluminum chloride or iron sulfate but am not sure. Looking to help coagulate hydroxides from a sodium hydroxide solution that was used to strip soder mask from some pcb boards, expect most hydroxides present to be tin and lead. Any thoughts would be appreciated.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3695
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Online


[*] posted on 14-9-2019 at 21:20


I do not think that there will be lead hydroxide or tin hydroxide present,
sodium stannate https://en.wikipedia.org/wiki/Sodium_stannate
and
lead(II) oxide https://en.wikipedia.org/wiki/Lead(II)_oxide
are more likely.

Sorry, I have no idea what to use as a flocculant




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
a11051605
Harmless
*




Posts: 21
Registered: 25-8-2017
Member Is Offline

Mood: No Mood

[*] posted on 15-9-2019 at 18:36


Ah maybe, ya maybe the sodium stannate is possible, looking how to salvage any metals in solution or that have precipitated out of the lye solution. Suspect main metals present are lead, tin, and maybe a little silver in various forms of oxide or hydroxide from the sodium hydroxide solution. Lots of literature on how to process acid waste but hardly anything on bases.
View user's profile View All Posts By User
happyfooddance
National Hazard
****




Posts: 530
Registered: 9-11-2017
Location: Los Angeles, Ca.
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2019 at 11:22


You haven't indicated the concentration of your lye solution or its known/suspected Pb/Zn content, but activated carbon should work. Bases stick to carbon pretty well, though, and a high concentration of lye will surely make it less efficient. You can filter the carbon and burn it (fumes!) to recover your metals.

With acidic solutions metal recovery is usually done with electrolysis. Depending on your process needs and how much zinc you have, that might be easiest way for that one.
View user's profile View All Posts By User
a11051605
Harmless
*




Posts: 21
Registered: 25-8-2017
Member Is Offline

Mood: No Mood

[*] posted on 16-9-2019 at 19:01


The concentration of the lye solution is around 1.75 to 1.5 mole. Have 2 pounds of lye dissolve in 4 gallons of water with additional 1950 ml of 12% hydrogen peroxide. Unknown quantity of metals in solution.